A COMPARISON OF U-BEND AND SLOW STRAIN RATE PROCEDURES FOR ASSESSING THE SCC RESISTANCE OF TYPE-304 STAINLESS-STEEL IN HIGH-TEMPERATURE WATER

被引:11
作者
YANG, W [1 ]
ZHANG, M [1 ]
ZHAO, G [1 ]
CONGLETON, J [1 ]
机构
[1] UNIV NEWCASTLE UPON TYNE,DEPT MECH MAT & MFG ENGN,DIV MAT,NEWCASTLE TYNE NE1 7RU,TYNE & WEAR,ENGLAND
关键词
AUGER ELECTRON SPECTROSCOPY; HIGH-TEMPERATURE WATER; SLOW STRAIN RATE TESTS; STAINLESS STEEL; STRESS CORROSION CRACKING; U-BEND;
D O I
10.5006/1.3585249
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of temperature, chloride content, and dissolved oxygen content on the susceptibility to stress corrosion cracking (SCC) of type 304 stainless steel in high-temperature water have been investigated. Both U-bend and slow strain rate stress corrosion tests were performed, complemented by electrochemical polarization curve measurements and extensive oxide film analyses by Auger electron spectroscopy (AES). The U-bend data showed decreasing susceptibility to cracking with increasing temperature, which correlated with thicker oxide films and greater enrichment of chromium in the films. In contrast, the slow strain rate tests (SSRTs) indicated maximum susceptibility to cracking at 250-degrees-C in the temperature range 200 to 300-degrees-C and the susceptibility to cracking increased with increasing oxide thickness. The extent of chromium and nickel enhancement in the oxide layers were different for the two specimen types tested in equivalent environments. Greater enhancement of nickel occurred in films formed on SSRT specimens than on U-bend specimens. It is concluded that the choice of test procedure for acquiring accelerated test data may be influenced by whether the components to which the data will be applied are likely to experience plastic strain during use.
引用
收藏
页码:226 / 233
页数:8
相关论文
共 25 条
[11]   EFFECT OF OXYGEN TEMPERATURE COMBINATIONS ON THE STRESS-CORROSION SUSCEPTIBILITY OF SENSITIZED TYPE-304 STAINLESS-STEEL IN HIGH-PURITY WATER [J].
FORD, FP ;
POVICH, MJ .
CORROSION, 1979, 35 (12) :569-574
[12]  
GORDON BM, 1980, MATER PERFORMANCE, V19, P29
[13]   ELECTROMOTIVE FORCE STUDIES IN AQUEOUS SOLUTIONS AT ELEVATED TEMPERATURES .1. THE STANDARD POTENTIAL OF THE SILVER-SILVER CHLORIDE ELECTRODE [J].
GREELEY, RS ;
SMITH, WT ;
STOUGHTON, RW ;
LIETZKE, MH .
JOURNAL OF PHYSICAL CHEMISTRY, 1960, 64 (05) :652-657
[14]   THE EFFECT OF DISSOLVED-OXYGEN AND NO3- ANIONS ON THE STRESS-CORROSION CRACKING OF TYPE-304 STAINLESS-STEEL IN WATER AT 290-C [J].
HIRANO, H ;
AOKI, N ;
KUROSAWA, T .
CORROSION, 1983, 39 (08) :313-322
[15]  
HIRANO H, 1982, BOSHOKU GIJUTSU, V31, P517
[16]  
HIRANO H, 1985, BOSHOKU GIJUTSU, V34, P92
[17]  
HIRAYAMA H, 1985, BOSHOKU GIJUTSU, V34, P86
[18]   HIGH-TEMPERATURE ELECTROCHEMICAL STUDIES OF THE STRESS-CORROSION OF TYPE-304 STAINLESS-STEEL [J].
INDIG, ME ;
MCILREE, AR .
CORROSION, 1979, 35 (07) :288-295
[19]   EFFECTS OF ENVIRONMENTAL-FACTORS ON PROGRESS OF STRESS-CORROSION CRACKS OF TYPE-304 STAINLESS-STEEL IN HIGH-TEMPERATURE WATER [J].
ISHIHARA, T ;
MATSUSHIMA, S ;
OHASHI, S ;
SHIMIZU, Y .
JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1977, 41 (06) :596-601
[20]  
ISHIHARA T, 1953, BOSHOKU GIJUTSU, V32, P324