X-RAY CREATION AND ACTIVATION OF ELECTRON-SPIN-RESONANCE IN VITREOUS SILICA

被引:78
作者
GALEENER, FL [1 ]
KERWIN, DB [1 ]
MILLER, AJ [1 ]
MIKKELSEN, JC [1 ]
机构
[1] XEROX CORP, PALO ALTO RES CTR, PALO ALTO, CA 94304 USA
关键词
D O I
10.1103/PhysRevB.47.7760
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
We report strong dependencies of electron-spin-resonance (ESR) signals in fused silica on x-ray dose, sample hydroxyl concentration [OH], and preirradiation sample-annealing temperature T(F). In general, the strengths of the E'-center ESR signal and the two oxgyen-hole-center signals increase nonlinearly with Cu-target x-ray dose; we ascribe this behavior to the coexistence of two processes: (1) The x-ray activation of the spins of pre-existing structural defects, and (2) the x-ray creation of new similar defects. From this model and the observed nonlinear dependence on dose, we obtain relative values for the number of pre-existing defects, their rate of activation by x rays, and the rate of creation of new defects. These relative values are then examined for their trends with respect to [OH] and T(F): For example, there are far more pre-existing E' precursor defects in ''dry'' Suprasil-W1 ([OH] < 2 ppm) than in ''wet'' Suprasil- 1 ([OH] almost-equal-to 1200 ppm) fused silica, yet new E' defects are about twice as easy to create with x rays in the ''wet'' material. In general, we find that the relative x-radiation ''hardness'' of different fused silica samples is strongly dependent on dose, hydroxyl content, and thermal history. From the [OH] and T(F) dependencies of spin concentrations, we conclude that none of the three spin-active defects can be identified with either of the two previously reported Raman-active defects, traditionally labeled D1 and D2. Moreover, we conclude that D2 is not a strongly preferential site for formation of the spin-active defects under x irradiation, and that D1 is unlikely to be such a site.
引用
收藏
页码:7760 / 7779
页数:20
相关论文
共 108 条
[101]   PARAMAGNETIC RESONANCE OF LATTICE DEFECTS IN IRRADIATED QUARTZ [J].
WEEKS, RA .
JOURNAL OF APPLIED PHYSICS, 1956, 27 (11) :1376-1381
[102]   TRAPPED ELECTRONS IN IRRADIATED QUARTZ AND SILICA .2. ELECTRON SPIN RESONANCE [J].
WEEKS, RA ;
NELSON, CM .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1960, 43 (08) :399-404
[103]   IRRADIATION EFFECTS AND SHORT-RANGE ORDER IN FUSED SILICA AND QUARTZ [J].
WEEKS, RA ;
NELSON, CM .
JOURNAL OF APPLIED PHYSICS, 1960, 31 (09) :1555-1558
[104]   RELATION BETWEEN E] CENTERS + HYDROXYL BONDS IN SILICA [J].
WEEKS, RA ;
LELL, E .
JOURNAL OF APPLIED PHYSICS, 1964, 35 (06) :1932-&
[105]   ELECTRON SPIN RESONANCE OF IRRADIATED QUARTZ - ATOMIC HYDROGEN [J].
WEEKS, RA ;
ABRAHAM, M .
JOURNAL OF CHEMICAL PHYSICS, 1965, 42 (01) :68-&
[106]  
WEEKS RA, 1967, INTERACTION RAD SOLI, P55
[107]  
Wong J., 1977, GLASS STRUCTURE SPEC
[108]  
[No title captured]