Reliability of thermally oxidized SiO2/4H-SiC by conductive atomic force microscopy

被引:28
作者
Fiorenza, Patrick [1 ]
Raineri, Vito [1 ]
机构
[1] CNR, IMM, I-95121 Catania, Italy
关键词
Atomic force microscopy - Electric potential - Epitaxial growth - MOS devices - Oxidation - Silica - Thermal effects;
D O I
10.1063/1.2207991
中图分类号
O59 [应用物理学];
学科分类号
摘要
The dielectric breakdown (BD) kinetics of silicon dioxide (SiO2) thin films thermally grown on 4H-SiC was determined by comparison between I-V measurements on large area (up to 1.96 x 10(-5) cm(2)) metal-oxide-semiconductor structures and conductive atomic force microscopy (C-AFM). C-AFM clearly images the weak breakdown single spots under constant voltage stresses. The stress time on the single C-AFM tip dot was varied from 2.5 x 10(-3) to 1 x 10(-1) s. The density of BD spots, upon increasing the stress time, exhibits an exponential trend. The Weibull slope and the characteristic time of the dielectric BD events have been determined by direct measurements at nanometer scale allowing to demonstrate that the percolative model is valid for thermal oxide on 4H-SiC. (c) 2006 American Institute of Physics.
引用
收藏
页数:3
相关论文
共 13 条
[11]   Percolation models for gate oxide breakdown [J].
Stathis, JH .
JOURNAL OF APPLIED PHYSICS, 1999, 86 (10) :5757-5766
[12]   Steam-induced interface improvement of N2O-nitrided SiO2 grown on 6H-SiC [J].
Xu, JP ;
Lai, PT ;
Chan, CL .
SOLID-STATE ELECTRONICS, 2003, 47 (08) :1397-1400
[13]   Study of carbon in thermal oxide formed on 4H-SiC by XPS [J].
Zhao, P ;
Rusli ;
Xia, JH ;
Tan, CM ;
Liu, Y ;
Tin, CC ;
Yoon, SF ;
Zhu, WG ;
Ahn, J .
SILICON CARBIDE AND RELATED MATERIALS 2004, 2005, 483 :653-656