Deposition and characterization of ternary thin films within the Ti-Al-C system by DC magnetron sputtering

被引:231
作者
Wilhelmsson, O.
Palmquist, J. -P.
Lewin, E.
Emmerlich, J.
Eklund, P.
Persson, P. O. A.
Hogberg, H.
Li, S.
Ahuja, R.
Eriksson, O.
Hultman, L.
Jansson, U.
机构
[1] Uppsala Univ, Angstrom Lab, Dept Chem Mat, SE-75121 Uppsala, Sweden
[2] Linkoping Univ, Thin Film Phys Div, IFM, Dept Phys, SE-58183 Linkoping, Sweden
[3] Uppsala Univ, Angstrom Lab, Dept Phys, SE-75121 Uppsala, Sweden
关键词
solid solutions; PVD; carbides; MAX-phase; perovksite;
D O I
10.1016/j.jcrysgro.2006.03.008
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
The formation of ternary compounds within the Ti-Al-C system was studied by magnetron sputtering for thin-film deposition and first-principles calculations for phase stability. As-deposited films were characterized with X-ray diffraction (XRD) and high-resolution transmission electron microscopy (TEM). The hardness and Young's moduli of the material were studied by nanoindentation. Epitaxial and phase-pure films of M(n+1)AX(n) phases Ti3AlC2 and Ti2AlC as well as the perovskite phase Ti3AlC were deposited on Al2O3(00l) wafers kept at temperatures between 800 and 900 degrees C. The only ternary phases observed at low temperatures (300 degrees C) were Ti3AlC and cubic (Ti,Al)C, the latter can be described as a metastable solid solution of Al in TiC similar to the more studied (Ti,Al)N system. The difficulties to form MAX phases at low substrate temperatures were attributed of requirement for a sufficient diffusivity to partition the elements corresponding to the relatively complex crystal structures with long c-axes. While MAX-phase synthesis at 800 degrees C is significantly lower than contemporary bulk sintering processes, a reduction of the substrate temperature towards 300 degrees C in the present thin-film deposition experiments resulted in stacking sequence variations and the intergrowth of (Ti,AI)C. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:290 / 300
页数:11
相关论文
共 49 条
[31]  
SAMIR FM, 1997, J MATER CHEM, V7, P99
[32]   Analysis of the indentation size effect in the microhardness measurement of some cobalt-based alloys [J].
Sangwal, K ;
Surowska, B ;
Blaziak, P .
MATERIALS CHEMISTRY AND PHYSICS, 2003, 77 (02) :511-520
[33]   XPS, AFM and nanoindentation studies of Ti1-xAlxN films synthesized by reactive unbalanced magnetron sputtering [J].
Shum, PW ;
Zhou, ZF ;
Li, KY ;
Shen, YG .
MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2003, 100 (02) :204-213
[34]   High temperature oxidation behavior of Ti3SiC2-based material in air [J].
Sun, Z ;
Zhou, Y ;
Li, M .
ACTA MATERIALIA, 2001, 49 (20) :4347-4353
[35]   Bonding and classification of nanolayered ternary carbides [J].
Sun, ZM ;
Music, D ;
Ahuja, R ;
Li, S ;
Schneider, JM .
PHYSICAL REVIEW B, 2004, 70 (09) :092102-1
[36]   Structure and bulk modulus of M2AlC (M=Ti, V, and Cr) [J].
Sun, ZM ;
Ahuja, R ;
Li, S ;
Schneider, JM .
APPLIED PHYSICS LETTERS, 2003, 83 (05) :899-901
[37]  
TIAN WH, 1996, INTERMET, V5, P237
[38]  
Toth L. E., 1971, TRANSITION METAL CAR
[39]   Synthesis and characterization of Ti3AlC2 [J].
Tzenov, NV ;
Barsoum, MW .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2000, 83 (04) :825-832
[40]  
Villars P. Pierre, 1995, HDB TERNARY ALLOY PH, V4