The character of dislocations in LiCoO2

被引:80
作者
Gabrisch, H [1 ]
Yazami, R
Fultz, B
机构
[1] CALTECH, Div Engn & Appl Sci, Pasadena, CA 91125 USA
[2] Inst Natl Polytech Grenoble, Lab Electrochim & Physicochim Mat Interface, CNRS, UMR 5631, F-38402 St Martin Dheres, France
关键词
D O I
10.1149/1.1472257
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Dislocations in LiCoO2 were observed by transmission electron microscopy, and their Burgers vectors were determined by analysis of diffraction contrast in tilting experiments. The configuration of all dislocations indicates that they are glissile, and dislocation configurations were found that are indicative of active slip planes. Perfect dislocations of a/3 [11 (2) over bar0] type Burgers vectors were observed on {0001} habit planes. These perfect dislocations sometimes dissociate into Shockley partial dislocations with a/3[10 (1) over bar0] type Burgers vectors. Glide of these partial dislocations can account for the sequence of crystal structures O3, H1-3, O1 that occur with the delithiation of LiCoO2. The presence of glissile dislocations also suggests possible damage mechanisms during cycling. (C) 2002 The Electrochemical Society.
引用
收藏
页码:A111 / A114
页数:4
相关论文
共 15 条
[1]   CoO2, the end member of the LixCoO2 solid solution [J].
Amatucci, GG ;
Tarascon, JM ;
Klein, LC .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1996, 143 (03) :1114-1123
[2]   Lithium insertion into host materials: the key to success for Li ion batteries [J].
Broussely, M ;
Biensan, P ;
Simon, B .
ELECTROCHIMICA ACTA, 1999, 45 (1-2) :3-22
[3]  
DELANOT MF, 1989, J MATER SCI, V24, P1594
[4]  
DELMAS C, 1994, LITHIUM BATTERIES NE, P457
[5]  
EDINGTON JW, 1976, PRACTICAL ELECT MICR, P87
[6]  
Goodenough J. B., 1998, LITHIUM ION BATTERIE, P1
[7]  
Hirth J. P., 1982, THEORY DISLOCATIONS, P315
[8]   Stacking faults and phase transformations in silicon nitride [J].
Milhet, X ;
Demenet, JL ;
Rabier, J .
EUROPEAN PHYSICAL JOURNAL-APPLIED PHYSICS, 1998, 4 (02) :149-156
[9]   SOLID-STATE REDOX REACTIONS OF LICOO2 (R(3)OVER-BAR-M) FOR 4 VOLT SECONDARY LITHIUM CELLS [J].
OHZUKU, T ;
UEDA, A .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1994, 141 (11) :2972-2977
[10]  
PARTRIDGE PG, 1967, MET REV, V12, P118