摘要
Anodizing of magnesium was studied in solutions containing 3 M KOH + 0.6 M KF + 0.21 M Na3PO4, with and without addition of 0.4 M and 1.1 M of aluminate. At constant applied current, the process occurs in two stages. First, the voltage rises linear ly until an initial breakdown occurs. A thin and compact oxide film is formed at this stage. In the second stage an intense continuous spark is maintained on the metal surface. A thick oxide film is formed at the site of sparking. The formation of the film is accompanied by voltage oscillation and gas evolution. The anodic films formed under continuous breakdown conditions are rough and porous and enriched in aluminum. Anodic films formed in a bath containing 1.1 M aluminate at 15 mA/cm(2) are composed of a single oxide phase MgAl2O4 spinel. (C) 1999 The Electrochemical Society. S0013-4651(98)09-036-3. All rights reserved.
引用
收藏
页码:1757 / 1761
页数:5
相关论文
共 20 条
[1]  
Emley EF., 1966, PRINCIPLES MAGNESIUM
[2]  
EVANGELIDES HA, 1951, MET FINISH, V7, P56
[3]  
Gruss L.L., 1963, ELECTROCHEM TECHNOL, V1, P283
[5]  
IKONOPISOV S, 1977, ELECTROCHIM ACTA, V22, P207
[6]   The anodic behavior of binary Mg-Al alloys in KOH-aluminate solutions [J].
Khaselev, O ;
Yahalom, J .
CORROSION SCIENCE, 1998, 40 (07) :1149-1160
[7]   Constant voltage anodizing of Mg-Al alloys in KOH-Al(OH)3 solutions [J].
Khaselev, O ;
Yahalom, J .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1998, 145 (01) :190-193
[8]  
KING JF, 1972, 7751978 US NAT TECH
[9]   ELECTRICAL BREAKDOWN .2. DURING THE ANODIC GROWTH OF ALUMINUM-OXIDE [J].
KLEIN, N ;
MOSKOVICI, V ;
KADARY, V .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1980, 127 (01) :152-155
[10]  
McNeill W., 1955, MET FINISH, V53, P57