Development of an extremely wear-resistant ultra high molecular weight polyethylene for total hip replacements

被引:569
作者
McKellop, H
Shen, FW
Lu, B
Campbell, P
Salovey, R
机构
[1] Orthoped Hosp, Res Adm Off, Joint Replacement Inst, Los Angeles, CA 90007 USA
[2] Univ So Calif, J Vernon Luck Orthopaed Res Ctr, Los Angeles, CA USA
[3] Univ So Calif, Dept Orthopaed, Los Angeles, CA USA
[4] Univ So Calif, Dept Biomed Engn, Los Angeles, CA 90089 USA
[5] Univ So Calif, Dept Mat Sci, Los Angeles, CA 90089 USA
关键词
D O I
10.1002/jor.1100170203
中图分类号
R826.8 [整形外科学]; R782.2 [口腔颌面部整形外科学]; R726.2 [小儿整形外科学]; R62 [整形外科学(修复外科学)];
学科分类号
摘要
Osteolysis induced by ultra high molecular weight polyethylene wear debris is one of the primary factors limiting the lifespan of total hip replacements. Crosslinking polyethylene is known to improve its wear resistance in certain industrial applications, and crosslinked polyethylene acetabular cups have shown improved wear resistance in two clinical studies. In the present study, crosslinked polyethylene cups were produced by two methods. Chemically crosslinked cups were produced by mixing a peroxide with ultra high molecular weight polyethylene powder and then molding the cups directly to shape. Radiation-crosslinked cups were produced by exposing conventional extruded ultra high molecular weight polyethylene bar stock to gamma radiation at various doses from 3.3 to 100 Mrad (1 Mrad = 10 kGy), remelting the bars to extinguish residual free radicals (i.e., to minimize long-term oxidation), and then machining the cups by conventional techniques. In hip-joint simulator tests lasting as long as 5 million cycles, both types of crosslinked cups exhibited dramatically improved resistance to wear. Artificial aging of the cups by heating for 30 days in air at 80 degrees C induced oxidation of the chemically crosslinked cups. However, a chemically crosslinked cup that was aged 2.7 years at room temperature had very little oxidation. Thus, whether substantial oxidation of chemically crosslinked polyethylene would occur at body temperature remains unclear. The radiation-crosslinked remelted cups exhibited excellent resistance to oxidation. Because crosslinking can reduce the ultimate tensile strength, fatigue strength, and elongation to failure of ultra high molecular weight polyethylene, the optimal crosslinking dose provides a balance between these physical properties and the wear resistance of the implant and might substantially reduce the incidence of wear-induced osteolysis with total hip replacements.
引用
收藏
页码:157 / 167
页数:11
相关论文
共 51 条
[31]   EXPLORATORY INVESTIGATIONS ON THE STRUCTURE DEPENDENCE OF THE WEAR-RESISTANCE OF POLYETHYLENE [J].
ROSE, RM ;
CIMINO, WR ;
ELLIS, E ;
CRUGNOLA, AN .
WEAR, 1982, 77 (01) :89-104
[32]   PERIPROSTHETIC BONE LOSS IN TOTAL HIP-ARTHROPLASTY - POLYETHYLENE WEAR DEBRIS AND THE CONCEPT OF THE EFFECTIVE JOINT SPACE [J].
SCHMALZRIED, TP ;
JASTY, M ;
HARRIS, WH .
JOURNAL OF BONE AND JOINT SURGERY-AMERICAN VOLUME, 1992, 74A (06) :849-863
[33]   Quantitative assessment of walking activity after total hip or knee replacement [J].
Schmalzried, TP ;
Szuszczewicz, ES ;
Northfield, MR ;
Akizuki, KH ;
Frankel, RE ;
Belcher, G ;
Amstutz, HC .
JOURNAL OF BONE AND JOINT SURGERY-AMERICAN VOLUME, 1998, 80A (01) :54-59
[34]  
Shen FW, 1998, J BIOMED MATER RES, V41, P71, DOI 10.1002/(SICI)1097-4636(199807)41:1<71::AID-JBM9>3.3.CO
[35]  
2-6
[36]  
Shen FW, 1996, J POLYM SCI POL PHYS, V34, P1063, DOI 10.1002/(SICI)1099-0488(19960430)34:6<1063::AID-POLB4>3.0.CO
[37]  
2-Z
[38]  
SHEN FW, 1994, THESIS LOS ANGELES U
[39]  
STREICHER RM, 1988, PLAST RUB PROC APPL, V10, P221
[40]  
STREICHER RM, 1989, BETA GAMMA, V1, P34