Strategies for the replacement of chromic acid anodising for the structural bonding of aluminium alloys

被引:136
作者
Critchlow, GW [1 ]
Yendall, KA
Bahrani, D
Quinn, A
Andrews, F
机构
[1] Univ Loughborough, Inst surface Sci & Technol, IPTME, Loughborough LE11 3TU, Leics, England
[2] Short Bros Bombardier Aerosp, Belfast BT3 9DZ, Antrim, North Ireland
[3] Thales Air Def, Belfast, Antrim, North Ireland
关键词
aluminium; surface treatment by chemical solutions; microscopy; durability;
D O I
10.1016/j.ijadhadh.2005.07.001
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The 40/50V Bengough-Stuart chromic acid anodise process is widely used in demanding applications as a prebond treatment. This process has a number of disadvantages and its replacement is the subject of much interest in the aerospace, automotive and defence sectors, amongst others. This paper details a number of modifications to the standard boric-sulphuric acid anodising (BSAA) process specifically to achieve satisfactory structural bond performance. These included: variations in the deoxidiser and anodising parameters; and the use of a post-anodising dip. It has been demonstrated in these studies that there are three possible methods of providing excellent durability using a variation of the standard BSAA process: the use of an electrolytic phosphoric acid deoxidiser; a high temperature anodise at 35 degrees C; and the use of a post-anodise phosphoric acid dip. (C) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:419 / 453
页数:35
相关论文
共 126 条
[31]   Further studies into the effectiveness of CO2-laser treatment of metals for adhesive bonding [J].
Critchlow, GW ;
Cottam, CA ;
Brewis, DM ;
Emmony, DC .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 1997, 17 (02) :143-150
[32]   An environmentally-friendly process for bonding aluminum using aqueous metasilicate sol-gel and silane adhesion promoters [J].
Crook, RA ;
Sinclair, JW ;
Poulter, LW ;
Schulte, KJ .
JOURNAL OF ADHESION, 1998, 68 (3-4) :315-+
[33]   Characteristics of weld-bonded commercial aluminum sheets (BS 1050) [J].
Darwish, SM .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2003, 23 (03) :169-176
[34]  
Dasquet JP, 1999, COMP EXPTL METHODS, V3, P149
[35]  
Davis GD, 1997, SURF INTERFACE ANAL, V25, P366, DOI 10.1002/(SICI)1096-9918(199705)25:5<366::AID-SIA245>3.0.CO
[36]  
2-S
[37]   APPLICATION OF SURFACE BEHAVIOR DIAGRAMS TO THE STUDY OF HYDRATION OF PHOSPHORIC-ACID ANODIZED ALUMINUM [J].
DAVIS, GD ;
SUN, TS ;
AHEARN, JS ;
VENABLES, JD .
JOURNAL OF MATERIALS SCIENCE, 1982, 17 (06) :1807-1818
[38]  
*DEF STAN, 1996, 03243 DEF STAN
[39]   The fatigue and durability behaviour of automotive adhesives. Part II: Failure mechanisms [J].
Dickie, RA ;
Haack, LP ;
Jethwa, JK ;
Kinloch, AJ ;
Watts, JF .
JOURNAL OF ADHESION, 1998, 66 (1-4) :1-+
[40]   PRETREATMENT OF ALUMINUM - TOPOGRAPHY, SURFACE-CHEMISTRY AND ADHESIVE BOND DURABILITY [J].
DIGBY, RP ;
PACKHAM, DE .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 1995, 15 (02) :61-71