Growth and structural characterization of yttria-stabilized zirconia-gold nanocomposite films with improved toughness

被引:92
作者
Voevodin, AA [1 ]
Hu, JJ [1 ]
Jones, JG [1 ]
Fitz, TA [1 ]
Zabinski, JS [1 ]
机构
[1] USAF, Res Lab, MLBT, Mat & Mfg Directorate, Wright Patterson AFB, OH 45433 USA
关键词
zirconium oxide; gold; composite; nanostructures;
D O I
10.1016/S0040-6090(01)01615-7
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To counteract the natural brittleness of oxide ceramic films and achieve better toughness, nanocomposite films combining yttria-stabilized zirconia (YSZ) and gold were produced. A hybrid of magnetron sputtering and pulsed laser ablation was used to grow crystalline YSZ embedded in an amorphous YSZ/Au matrix at near room temperature. Results from chemical analyses, Xray and electron diffraction, high-resolution transmission electron microscopy, lateral force microscopy, nanoindentation hardness measurements and toughness estimates are discussed. At a fixed deposition temperature, the film microstructure was critically dependent on the gold content. Three distinct microstructures were produced: an amorphous YSZ/Au coating at less than 8 at.% Au; 5-10 mn YSZ crystals embedded in an amorphous YSZ/Au matrix at 10-15 at.% Au; and 20-100-nm crystallites of (101)-oriented YSZ mixed with micron-sized Au agglomerates at above 20 at.% Au. From these films, only the 5-10 nm nanocrystalline YSZ embedded in the amorphous YSZ/Au matrix provided the improvements in toughness. Coatings with this structure had hardness of 15-20 GPa, elastic modulus of approximately 250 GPa, and did not develop cracks in Vickers pyramid indentation at loads up to I kg, showing remarkable ductility. The improvement in toughness of this relatively hard film was explained by grain boundary sliding of YSZ nanocrystals in the YSZ/Au amorphous matrix. The new YSZ/Au nanocomposite films developed in this study may have good potential for surface protection, where a combination of thermal stability, oxidation resistance and improved film toughness are required. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:187 / 195
页数:9
相关论文
共 46 条
[21]  
Mitterer C, 1999, Z METALLKD, V90, P602
[22]   Microstructural effects on the friction and wear of zirconia films in unlubricated sliding contact [J].
Moulzolf, SC ;
Lad, RJ ;
Blau, PJ .
THIN SOLID FILMS, 1999, 347 (1-2) :220-225
[23]   Hard and superhard nanocomposite coatings [J].
Musil, J .
SURFACE & COATINGS TECHNOLOGY, 2000, 125 (1-3) :322-330
[24]   AN IMPROVED TECHNIQUE FOR DETERMINING HARDNESS AND ELASTIC-MODULUS USING LOAD AND DISPLACEMENT SENSING INDENTATION EXPERIMENTS [J].
OLIVER, WC ;
PHARR, GM .
JOURNAL OF MATERIALS RESEARCH, 1992, 7 (06) :1564-1583
[25]   AVERAGE ENERGY DEPOSITED PER ATOM - A UNIVERSAL PARAMETER FOR DESCRIBING ION-ASSISTED FILM GROWTH [J].
PETROV, I ;
ADIBI, F ;
GREENE, JE ;
HULTMAN, L ;
SUNDGREN, JE .
APPLIED PHYSICS LETTERS, 1993, 63 (01) :36-38
[26]   Microtribological behavior of Au(001) studied by AFM/FFM [J].
Polaczyk, C ;
Schneider, T ;
Schofer, J ;
Santner, E .
SURFACE SCIENCE, 1998, 402 (1-3) :454-458
[27]   Quantitative analysis of the frictional properties of solid materials at low loads .1. Carbon compounds [J].
Schwarz, UD ;
Zworner, O ;
Koster, P ;
Wiesendanger, R .
PHYSICAL REVIEW B, 1997, 56 (11) :6987-6996
[28]   COATINGS FOR WEAR AND LUBRICATION [J].
SPALVINS, T .
THIN SOLID FILMS, 1978, 53 (03) :285-300
[29]  
Tamayo J, 1996, APPL PHYS LETT, V68, P2297, DOI 10.1063/1.116169