Enzyme catalysis of alumina forming

被引:31
作者
Gauckler, LJ [1 ]
Graule, TJ [1 ]
Baader, FH [1 ]
Will, J [1 ]
机构
[1] ETH Zurich, Dept Mat, Nichtmet Werkstoffe, CH-8092 Zurich, Switzerland
来源
NOVEL SYNTHESIS AND PROCESSING OF CERAMICS | 1999年 / 159-1卷
关键词
ceramics; green body; manufacturing; high strength high reliability; colloidal forming; enzyme catalyzed reactions; coagulation casting;
D O I
10.4028/www.scientific.net/KEM.159-160.135
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this work we describe a new ceramic green body fabrication method using ceramic colloidal suspensions that allow the production of complex shaped parts of high strength and reliability. The method uses an aqueous, electrostatically stabilized ceramic suspension free of agglomerates and of low viscosity. It is cast into a mold and then coagulates forming a stiff, wet green body. Coagulation is performed by changing the pH of the suspension and/or by creating salt directly inside the suspension using a controlled time-delayed reaction, Enzyme catalyzed reactions that are decomposing a substrate, or self-propagating decomposition reactions of a substrate, can be used. After the coagulation reaction in the suspension, the wet green body shows good mechanical properties and can be demolded, dried and sintered. This new forming process DCC (Direct Coagulation Casting) is characterized by near net shape capability of complex shaped parts with high quality and homogeneity in the green as well as in the sintered state. Only small amounts of organic additives which amount to less than 0.5 wt-% based on ceramic powder are needed for the catalytic reactions. Since the forming process takes place without pressure and at ambient temperatures, inexpensive molds and tools can be used. Ceramic bodies with homogeneous, defect poor microstructures can be cast using almost any ceramic powder. Complex shaped components with thin and thick cross sections can be cast as there is no gradient in density and/or temperature during consolidation of the green body. Alumina parts of average bend strength (680 MPa) and high reliability (Weibull-module m=40) have been demonstrated.
引用
收藏
页码:135 / 149
页数:15
相关论文
共 48 条
[21]   CONTROLLED DRUG RELEASE BY POLYMER DISSOLUTION .1. PARTIAL ESTERS OF MALEIC-ANHYDRIDE COPOLYMERS-PROPERTIES AND THEORY [J].
HELLER, J ;
BAKER, RW ;
GALE, RM ;
RODIN, JO .
JOURNAL OF APPLIED POLYMER SCIENCE, 1978, 22 (07) :1991-2009
[22]  
HELLER J, 1987, ACS SYM SER, V348, P172
[23]  
HERMAN MEA, 1970, 2770 RCMKEMA
[24]   Influence of the dispersant structure on properties of electrostatically stabilized aqueous alumina suspensions [J].
Hidber, PC ;
Graule, TJ ;
Gauckler, LJ .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1997, 17 (2-3) :239-249
[25]   Citric acid - A dispersant for aqueous alumina suspensions [J].
Hidber, PC ;
Graule, TJ ;
Gauckler, LJ .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (07) :1857-1867
[26]   COMPETITIVE ADSORPTION OF CITRIC-ACID AND POLY(VINYL ALCOHOL) ONTO ALUMINA AND ITS INFLUENCE ON THE BINDER MIGRATION DURING DRYING [J].
HIDBER, PC ;
GRAULE, TJ ;
GAUCKLER, LJ .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1995, 78 (07) :1775-1780
[27]   SURFACE FORCES AND THEIR ACTION IN CERAMIC MATERIALS [J].
HORN, RG .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (05) :1117-1135
[28]   CENTRIFUGAL SLIP CASTING OF ZIRCONIA (TZP) [J].
HUISMAN, W ;
GRAULE, T ;
GAUCKLER, LJ .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1994, 13 (01) :33-39
[29]  
INGVORSEN K, 1988, CIBA F SYMP, V140, P16
[30]   PREPARATION AND PERMEABILITY OF UREA-RESPONSIVE POLYMER MEMBRANE CONSISTING OF IMMOBILIZED UREASE AND POLY(AROMATIC CARBOXYLIC-ACID) [J].
ISHIHARA, K ;
MURAMOTO, N ;
FUJII, H ;
SHINOHARA, I .
JOURNAL OF POLYMER SCIENCE PART C-POLYMER LETTERS, 1985, 23 (10) :531-535