TOF-SIMS investigation of degradation pathways occurring in a variety of organic photovoltaic devices - the ISOS-3 inter-laboratory collaboration

被引:32
作者
Andreasen, Birgitta [1 ]
Tanenbaum, David M. [1 ,2 ]
Hermenau, Martin [3 ]
Voroshazi, Eszter [4 ,5 ]
Lloyd, Matthew T. [6 ]
Galagan, Yulia [7 ]
Zimmernann, Birger [8 ]
Kudret, Suleyman [9 ]
Maes, Wouter [9 ]
Lutsen, Laurence [10 ]
Vanderzande, Dirk [9 ]
Wuerfel, Uli [8 ]
Andriessen, Ronn [7 ]
Roesch, Roland [11 ]
Hoppe, Harald [11 ]
Teran-Escobar, Gerardo [12 ]
Lira-Cantu, Monica [12 ]
Rivaton, Agnes [13 ]
Uzunoglu, Guelsah Y. [14 ]
Germack, David S. [15 ]
Hosel, Markus [1 ]
Dam, Henrik F. [1 ]
Jorgensen, Mikkel [1 ]
Gevorgyan, Suren A. [1 ]
Madsen, Morten V. [1 ]
Bundgaard, Eva [1 ]
Krebs, Frederik C. [1 ]
Norrman, Kion [1 ]
机构
[1] Tech Univ Denmark, Dept Energy Convers & Storage, DK-4000 Roskilde, Denmark
[2] Pomona Coll, Dept Phys & Astron, Claremont, CA 91711 USA
[3] Tech Univ Dresden, Inst Angew Photophys, Arbeitsgrp Organ Solarzellen OSOL, D-01062 Dresden, Germany
[4] IMEC, B-3000 Louvain, Belgium
[5] Katholieke Univ Leuven, ESAT, B-3000 Louvain, Belgium
[6] Natl Renewable Energy Lab, Golden, CO 80401 USA
[7] Holst Ctr, NL-5656 AE Eindhoven, Netherlands
[8] Fraunhofer Inst Solar Energy Syst ISE, D-79110 Freiburg, Germany
[9] Hasselt Univ, WET OBPC, B-3590 Diepenbeek, Belgium
[10] Campus Univ Hasselt, IMOMEC Associated Lab, IMEC, B-3590 Diepenbeek, Belgium
[11] Ilmenau Univ Technol, Inst Phys, D-98693 Ilmenau, Germany
[12] ETSE, Lab Nanostruct Mat Photovolta Energy, Ctr Invest Nanociencia & Nanotecnol CSIC CIN2, E-08193 Bellaterra, Barcelona, Spain
[13] Univ Clermont Ferrand, Clermont Univ, LPMM, F-63000 Clermont Ferrand, France
[14] CNRS, LPMM, UMR6505, F-63177 Aubiere, France
[15] Brookhaven Natl Lab, Upton, NY 11973 USA
基金
新加坡国家研究基金会;
关键词
POLYMER SOLAR-CELLS; OXYGEN; MECHANISMS; STABILITY; LIFETIMES; WATER;
D O I
10.1039/c2cp41787a
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The present work is the fourth (and final) contribution to an inter-laboratory collaboration that was planned at the 3rd International Summit on Organic Photovoltaic Stability (ISOS-3). The collaboration involved six laboratories capable of producing seven distinct sets of OPV devices that were degraded under well-defined conditions in accordance with the ISOS-3 protocols. The degradation experiments lasted up to 1830 hours and involved more than 300 cells on more than 100 devices. The devices were analyzed and characterized at different points of their lifetimes by a large number of non-destructive and destructive techniques in order to identify specific degradation mechanisms responsible for the deterioration of the photovoltaic response. Work presented herein involves time-of-flight secondary ion mass spectrometry (TOF-SIMS) in order to study chemical degradation in-plane as well as in-depth in the organic solar cells. Various degradation mechanisms were investigated and correlated with cell performance. For example, photo-oxidation of the active material was quantitatively studied as a function of cell performance. The large variety of cell architectures used (some with and some without encapsulation) enabled valuable comparisons and important conclusions to be drawn on degradation behaviour. This comprehensive investigation of OPV stability has significantly advanced the understanding of degradation behaviour in OPV devices, which is an important step towards large scale application of organic solar cells.
引用
收藏
页码:11780 / 11799
页数:20
相关论文
共 30 条
[1]   Interaction of oxygen with conjugated polymers: Charge transfer complex formation with poly(3-alkylthiophenes) [J].
Abdou, MSA ;
Orfino, FP ;
Son, Y ;
Holdcroft, S .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1997, 119 (19) :4518-4524
[2]   Formation of metastable charges as a first step in photoinduced degradation in π-conjugated polymer: fullerene blends for photovoltaic applications [J].
Aguirre, A. ;
Meskers, S. C. J. ;
Janssen, R. A. J. ;
Egelhaaf, H. -J. .
ORGANIC ELECTRONICS, 2011, 12 (10) :1657-1662
[3]  
[Anonymous], SPIE PRESS MONOGRAPH
[4]   Solar cell efficiency tables (Version 38) [J].
Green, Martin A. ;
Emery, Keith ;
Hishikawa, Yoshihiro ;
Warta, Wilhelm ;
Dunlop, Ewan D. .
PROGRESS IN PHOTOVOLTAICS, 2011, 19 (05) :565-572
[5]   Oxygen doping-induced photogeneration loss in P3HT:PCBM solar cells [J].
Guerrero, Antonio ;
Boix, Pablo P. ;
Marchesi, Luis F. ;
Ripolles-Sanchis, Teresa ;
Pereira, Ernesto C. ;
Garcia-Belmonte, Germa .
SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2012, 100 :185-191
[6]   Water and oxygen induced degradation of small molecule organic solar cells [J].
Hermenau, Martin ;
Riede, Moritz ;
Leo, Karl ;
Gevorgyan, Suren A. ;
Krebs, Frederik C. ;
Norrman, Kion .
SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2011, 95 (05) :1268-1277
[7]   Stability/degradation of polymer solar cells [J].
Jorgensen, Mikkel ;
Norrman, Kion ;
Krebs, Frederik C. .
SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2008, 92 (07) :686-714
[8]   Stability of Polymer Solar Cells [J].
Jorgensen, Mikkel ;
Norrman, Kion ;
Gevorgyan, Suren A. ;
Tromholt, Thomas ;
Andreasen, Birgitta ;
Krebs, Frederik C. .
ADVANCED MATERIALS, 2012, 24 (05) :580-612
[9]  
Krebs F.C., 2012, STABILITY DEGRADATIO
[10]  
Krebs F.C., 2010, Polymer Solar Cells: Materials, Design, Manufacture