Vanadium oxide-PANI nanocomposite-based macroscopic fibers: 1D alcohol sensors bearing enhanced toughness

被引:52
作者
Dexmer, J. [2 ]
Leroy, C. M. [2 ]
Binet, L. [3 ]
Heresanu, V. [4 ]
Launois, P.
Steunou, N. [1 ]
Coulon, C. [2 ]
Maquet, J. [3 ]
Brun, N. [2 ]
Livage, J.
Backov, R. [2 ]
机构
[1] Univ Paris 06, UPMC, Coll France, CNRS,Lab Chim Mat Condensee Paris,UMR 7574, 4 Pl Jussieu, F-75252 Paris 05, France
[2] CNRS, Ctr Rech Paul Pascal, Off 115, UPR 8641, F-33600 Pessac, France
[3] CNRS, Ecole Natl Super Chim Paris, Lab Chim Mat Condensee Paris, UMR 7574, F-75005 Paris, France
[4] Univ Paris 11, Phys Solides Lab, CNRS, UMR 8502, F-91405 Orsay, France
关键词
D O I
10.1021/cm800886v
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
For the first time, using an extrusion process, macroscopic composite poly-vinyl alcohol (PVA)/polyaniline (PANI)-V2O5 fibers have been generated. Besides the extrusion process itself, this is certainly the first redox reaction addressed while performing an extrusion shaping process. The as-synthesized fibers have been characterized at different length scales, revealing at the mesoscale a 30 degrees preferential orientation of the nanoribbons subunits toward the macroscopic fiber main axis. At the microscopic length scale, despite a semiamorphous nature, electron spin resonance (ESR) spectroscopy has been employed to reveal partial reduction of V5+ species to V4+ ones, where the paramagnetic species local environment has been found to be close to hydrated vanadium Oxide xerogels. Concerning the organic counterpart, the aniline is oxidized into poly aniline when considering both the fibers characterization through ESR and Fourier transformed infrared (FTIR) spectroscopy and the well-known strongly oxidizing character of V5+ species toward aniline. These new PVA/PANI-V2O5 fibers are cycling when sensing alcoholic vapors while offering a good selectivity. The addressed sensitivity allows sensing 5 ppm of ethanol within 3-5 s at 42 degrees C. Beyond, the as-synthesized PVA/PANI-V2O5 macroscopic fibers possess a toughness of 12 J g(-1), a Value that has been increased by more than 120 times when compared with nanoporous inorganic C, fibers.
引用
收藏
页码:5541 / 5549
页数:9
相关论文
共 53 条
[11]   Influence of pH and ionic strength on vanadium(V) oxides formation.: From V2O5•nH2O gels to crystalline NaV3O8•1.5H2O [J].
Durupthy, O ;
Steunou, N ;
Coradin, T ;
Maquet, J ;
Bonhomme, C ;
Livage, J .
JOURNAL OF MATERIALS CHEMISTRY, 2005, 15 (10) :1090-1098
[12]   Millifluidic as a versatile reactor to tune size and aspect ratio of large polymerized objects [J].
Engl, W. ;
Tachibana, M. ;
Panizza, P. ;
Backov, R. .
INTERNATIONAL JOURNAL OF MULTIPHASE FLOW, 2007, 33 (08) :897-903
[13]   Monolithic mesoporous silica templated by microemulsion liquid crystals [J].
Feng, PY ;
Bu, XH ;
Stucky, GD ;
Pine, DJ .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2000, 122 (05) :994-995
[14]   Mesoporous and homothetic silica capsules in reverse-emulsion microreactors [J].
Fornasieri, G ;
Badaire, W ;
Backov, R ;
Mondain-Monval, O ;
Zakri, U ;
Poulin, P .
ADVANCED MATERIALS, 2004, 16 (13) :1094-+
[15]  
Gomez-Romero P, 2001, ADV MATER, V13, P163, DOI 10.1002/1521-4095(200102)13:3<163::AID-ADMA163>3.3.CO
[16]  
2-L
[17]   Synthesis, characterization, and conductivity studies of poly-o-methoxyaniline intercalated into V2O5 xerogel [J].
Guerra, EM ;
Brunello, CA ;
Graeff, CFO ;
Oliveira, HP .
JOURNAL OF SOLID STATE CHEMISTRY, 2002, 168 (01) :134-139
[18]   Morphosynthesis of complex inorganic forms using pollen grain templates [J].
Hall, SR ;
Bolger, H ;
Mann, S .
CHEMICAL COMMUNICATIONS, 2003, (22) :2784-2785
[19]   ESR in conducting polymers: Oxygen-induced contribution to the linewidth [J].
Houze, E ;
Nechtschein, M .
PHYSICAL REVIEW B, 1996, 53 (21) :14309-14318
[20]   Ordered macroporous materials by emulsion templating [J].
Imhof, A ;
Pine, DJ .
NATURE, 1997, 389 (6654) :948-951