Investigating the Dendritic Growth during Full Cell Cycling of Garnet Electrolyte in Direct Contact with Li Metal

被引:343
作者
Aguesse, Frederic [1 ]
Manalastas, William
Buannic, Lucienne
Lopez del Amo, Juan Miguel
Singh, Gurpreet
Llordes, Anna [1 ,2 ]
Kilner, John [3 ]
机构
[1] CIC Energigune, Parque Tecnol Alava,C Albert Einstein 48, Minano 01510, Spain
[2] Basque Fdn Sci, Ikerbasque, Maria Diaz de Haro 3, Bilbao 48013, Spain
[3] Imperial Coll London, Dept Mat, Exhibit Rd, London SW7 2AZ, England
关键词
garnet electrolyte; degradation mechanisms; dendritic lithium formation; full cell cycling; Li-metal/garnet interface; post mortem analysis; all-solid-state batteries; SITU NMR OBSERVATION; IN-SITU; ELECTROCHEMICAL PERFORMANCE; SOLID-ELECTROLYTE; LITHIUM; LI7LA3ZR2O12; CONDUCTIVITY; STABILITY; BATTERY; ALUMINA;
D O I
10.1021/acsami.6b13925
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
All-solid-state batteries including a garnet ceramic as electrolyte are potential candidates to replace the currently used Li-ion technology, as they offer safer Li metal operation and higher energy storage performances. However, the development of anode ceramic electrolyte batteries faces several challenges at the electrode/electrolyte interfaces, which need to withstand high current densities to enable competing Crates. In this work, we investigate the limits of the anode/electrolyte interface in a full cell that includes a Li-metal anode, LiFePO4 cathode, and garnet ceramic electrolyte. The addition of a liquid interfacial layer between the cathode and the ceramic electrolyte is found to be a prerequisite to achieve low interfacial resistance and to enable full use of the active material contained in the porous electrode. Reproducible and constant discharge capacities are extracted from the cathode active material during the first 20 cycles, revealing high efficiency of the garnet as electrolyte and the interfaces, but prolonged cycling leads to abrupt cell failure. By using a combination of structural and chemical characterization techniques, such as SEM and solid-state NMR, as well as electrochemical and impedance spectroscopy, it is demonstrated that a sudden impedance drop occurs in the cell due to the formation of metallic Li and its propagation within the ceramic electrolyte. This degradation process is originated at the interface between the Li-metal anode and the ceramic electrolyte layer and leads to electromechanical failure and cell short-circuit. Improvement of the performances is observed when cycling the full cell at 55 degrees C, as the Li-metal softening favors the interfacial contact. Various degradation mechanisms are proposed to explain this behavior.
引用
收藏
页码:3808 / 3816
页数:9
相关论文
共 40 条
[1]   Enhancement of the Grain Boundary Conductivity in Ceramic Li0.34La0.55TiO3 Electrolytes in a Moisture-Free Processing Environment [J].
Aguesse, Frederic ;
Lopez del Amo, Juan Miguel ;
Roddatis, Vladimir ;
Aguadero, Ainara ;
Kilner, John A. .
ADVANCED MATERIALS INTERFACES, 2014, 1 (07)
[2]   Modeling dendrite growth during lithium electrodeposition at sub-ambient temperature [J].
Akolkar, Rohan .
JOURNAL OF POWER SOURCES, 2014, 246 :84-89
[3]   Effect of substitution (Ta, Al, Ga) on the conductivity of Li7La3Zr2O12 [J].
Allen, J. L. ;
Wolfenstine, J. ;
Rangasamy, E. ;
Sakamoto, J. .
JOURNAL OF POWER SOURCES, 2012, 206 :315-319
[4]   In Situ Solid State 7Li NMR Observations of Lithium Metal Deposition during Overcharge in Lithium Ion Batteries [J].
Arai, J. ;
Okada, Y. ;
Sugiyama, T. ;
Izuka, M. ;
Gotoh, K. ;
Takeda, K. .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2015, 162 (06) :A952-A958
[5]   Building better batteries [J].
Armand, M. ;
Tarascon, J. -M. .
NATURE, 2008, 451 (7179) :652-657
[6]   Inorganic solid/organic liquid hybrid electrolyte for use in Li-ion battery [J].
Asl, Nina Mahootcheian ;
Keith, Joshua ;
Lim, Cheolwoong ;
Zhu, Likun ;
Kim, Youngsik .
ELECTROCHIMICA ACTA, 2012, 79 :8-16
[7]   Lithiation and Delithiation Mechanisms of Gold Thin Film Model Anodes for Lithium Ion Batteries: Electrochemical Characterization [J].
Bach, P. ;
Stratmann, M. ;
Valencia-Jaime, I. ;
Romero, A. H. ;
Renner, F. U. .
ELECTROCHIMICA ACTA, 2015, 164 :81-89
[8]   Atmosphere Controlled Processing of Ga-Substituted Garnets for High Li-Ion Conductivity Ceramics [J].
Bernuy-Lopez, Carlos ;
Manalastas, William, Jr. ;
Lopez del Amo, Juan Miguel ;
Aguadero, Ainara ;
Aguesse, Frederic ;
Kilner, John A. .
CHEMISTRY OF MATERIALS, 2014, 26 (12) :3610-3617
[9]  
Bhattacharyya R, 2010, NAT MATER, V9, P504, DOI [10.1038/nmat2764, 10.1038/NMAT2764]
[10]   Efficient Ion Exchange of H+ for Li+ in (Li0.30La0.57□0.13)TiO3 Perovskite in Water: Protons As a Probe for Li Location [J].
Boulant, Anthony ;
Maury, Pierre ;
Emery, Joel ;
Buzare, Jean-Yves ;
Bohnke, Odile .
CHEMISTRY OF MATERIALS, 2009, 21 (11) :2209-2217