Investigating the Dendritic Growth during Full Cell Cycling of Garnet Electrolyte in Direct Contact with Li Metal

被引:343
作者
Aguesse, Frederic [1 ]
Manalastas, William
Buannic, Lucienne
Lopez del Amo, Juan Miguel
Singh, Gurpreet
Llordes, Anna [1 ,2 ]
Kilner, John [3 ]
机构
[1] CIC Energigune, Parque Tecnol Alava,C Albert Einstein 48, Minano 01510, Spain
[2] Basque Fdn Sci, Ikerbasque, Maria Diaz de Haro 3, Bilbao 48013, Spain
[3] Imperial Coll London, Dept Mat, Exhibit Rd, London SW7 2AZ, England
关键词
garnet electrolyte; degradation mechanisms; dendritic lithium formation; full cell cycling; Li-metal/garnet interface; post mortem analysis; all-solid-state batteries; SITU NMR OBSERVATION; IN-SITU; ELECTROCHEMICAL PERFORMANCE; SOLID-ELECTROLYTE; LITHIUM; LI7LA3ZR2O12; CONDUCTIVITY; STABILITY; BATTERY; ALUMINA;
D O I
10.1021/acsami.6b13925
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
All-solid-state batteries including a garnet ceramic as electrolyte are potential candidates to replace the currently used Li-ion technology, as they offer safer Li metal operation and higher energy storage performances. However, the development of anode ceramic electrolyte batteries faces several challenges at the electrode/electrolyte interfaces, which need to withstand high current densities to enable competing Crates. In this work, we investigate the limits of the anode/electrolyte interface in a full cell that includes a Li-metal anode, LiFePO4 cathode, and garnet ceramic electrolyte. The addition of a liquid interfacial layer between the cathode and the ceramic electrolyte is found to be a prerequisite to achieve low interfacial resistance and to enable full use of the active material contained in the porous electrode. Reproducible and constant discharge capacities are extracted from the cathode active material during the first 20 cycles, revealing high efficiency of the garnet as electrolyte and the interfaces, but prolonged cycling leads to abrupt cell failure. By using a combination of structural and chemical characterization techniques, such as SEM and solid-state NMR, as well as electrochemical and impedance spectroscopy, it is demonstrated that a sudden impedance drop occurs in the cell due to the formation of metallic Li and its propagation within the ceramic electrolyte. This degradation process is originated at the interface between the Li-metal anode and the ceramic electrolyte layer and leads to electromechanical failure and cell short-circuit. Improvement of the performances is observed when cycling the full cell at 55 degrees C, as the Li-metal softening favors the interfacial contact. Various degradation mechanisms are proposed to explain this behavior.
引用
收藏
页码:3808 / 3816
页数:9
相关论文
共 40 条
[31]   In-situ, non-destructive acoustic characterization of solid state electrolyte cells [J].
Schmidt, Robert D. ;
Sakamoto, Jeffrey .
JOURNAL OF POWER SOURCES, 2016, 324 :126-133
[32]   Characterizing the Li-Li7La3Zr2O12 interface stability and kinetics as a function of temperature and current density [J].
Sharafi, Asma ;
Meyer, Harry M. ;
Nanda, Jagjit ;
Wolfenstine, Jeff ;
Sakamoto, Jeff .
JOURNAL OF POWER SOURCES, 2016, 302 :135-139
[33]   In situ NMR observation of the lithium extraction/insertion from LiCoO2 cathode [J].
Shimoda, Keiji ;
Murakami, Miwa ;
Takamatsu, Daiko ;
Arai, Hajime ;
Uchimoto, Yoshiharu ;
Ogumi, Zempachi .
ELECTROCHIMICA ACTA, 2013, 108 :343-349
[34]   NMR, DSC and high pressure electrical conductivity studies of liquid and hybrid electrolytes [J].
Stallworth, PE ;
Fontanella, JJ ;
Wintersgill, MC ;
Scheidler, CD ;
Immel, JJ ;
Greenbaum, SG ;
Gozdz, AS .
JOURNAL OF POWER SOURCES, 1999, 81 :739-747
[35]   Interface behavior between garnet-type lithium-conducting solid electrolyte and lithium, metal [J].
Sudo, R. ;
Nakata, Y. ;
Ishiguro, K. ;
Matsui, M. ;
Hirano, A. ;
Takeda, Y. ;
Yamamoto, O. ;
Imanishi, N. .
SOLID STATE IONICS, 2014, 262 :151-154
[36]   Garnet-type solid-state fast Li ion conductors for Li batteries: critical review [J].
Thangadurai, Venkataraman ;
Narayanan, Sumaletha ;
Pinzaru, Dana .
CHEMICAL SOCIETY REVIEWS, 2014, 43 (13) :4714-4727
[37]   Li7La3Zr2O12 Interface Modification for Li Dendrite Prevention [J].
Tsai, Chill-Long ;
Roddatis, Vladimir ;
Chandran, C. Vinod ;
Ma, Qianli ;
Uhlenbruck, Sven ;
Bram, Martin ;
Heitjans, Paul ;
Guillon, Olivier .
ACS APPLIED MATERIALS & INTERFACES, 2016, 8 (16) :10617-10626
[38]   DETERIORATION OF BETA''-ALUMINA CERAMICS UNDER ELECTROLYTIC CONDITIONS [J].
VIRKAR, AV ;
VISWANATHAN, L ;
BISWAS, DR .
JOURNAL OF MATERIALS SCIENCE, 1980, 15 (02) :302-308
[39]   Ionic Conductivity and Air Stability of Al-Doped Li7La3Zr2O12 Sintered in Alumina and Pt Crucibles [J].
Xia, Wenhao ;
Xu, Biyi ;
Duan, Huanan ;
Guo, Yiping ;
Kang, Hongmei ;
Li, Hua ;
Liu, Hezhou .
ACS APPLIED MATERIALS & INTERFACES, 2016, 8 (08) :5335-5342
[40]   The Birth of the Lithium-Ion Battery [J].
Yoshino, Akira .
ANGEWANDTE CHEMIE-INTERNATIONAL EDITION, 2012, 51 (24) :5798-5800