Apatite layer-coated titanium for use as bone bonding implants

被引:155
作者
Yan, WQ
Nakamura, T
Kawanabe, K
Nishigochi, S
Oka, M
Kokubo, T
机构
[1] KYOTO UNIV,FAC MED,DEPT ORTHOPAED SURG,SAKYO KU,KYOTO 606,JAPAN
[2] KYOTO UNIV,BIOMED ENGN RES CTR,KYOTO 606,JAPAN
[3] KYOTO UNIV,FAC ENGN,DEPT CHEM MAT,KYOTO 606,JAPAN
关键词
apatite layer; coating implant; biomimetic method; titanium; bone bonding;
D O I
10.1016/S0142-9612(97)00057-4
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
For development of thin bioactive coatings on metal implants, a dense and uniform apatite layer was coated onto titanium (Ti) implants in situ by using a new biomimetic method, which is composed of apatite nucleation and growth steps in simulated body fluid (SBF). Analysis of the coatings by thin film X-ray diffraction and scanning electron microscopy-energy dispersive X-ray microanalysis (SEM-EMPA) before implantation showed that its characteristics were very similar to those of natural bone. The coated and uncoated rectangular plates were bilaterally implanted into the tibial proximal metaphyses of rabbits. After 6, 10 and 25 weeks post-implantation, the bone bonding and bone formation at the bone-implant interfaces were evaluated by a detachment test and undecalcified histological examination. Mechanical testing in tension showed that the failure load of apatite layer-coated Ti implants was significantly higher than that of uncoated control at each time period (all P < 0.001). Histologically, it was shown that bone was deposited directly onto the apatite coating without any intervening soft tissue, while in the paired controls, interpositional soft tissue was seen at the bone-implant interface. By SEM-EPMA, a uniform calcium- and phosphorus-rich layer was detected between the coated implants and bone, but not in uncoated controls at either earlier or later time periods. The results indicate that the apatite layer deposited on Ti in situ may significantly increase the bone bonding strength by providing a bioactive surface, which allows for an early bone apposition to the implant. In addition, the apatite layer-coated Ti produced by the biomimetic process may fulfil the requirements of favourable thin coatings and strong adhesion at the metal-coating interface. (C) 1997 Elsevier Science Limited. All rights reserved.
引用
收藏
页码:1185 / 1190
页数:6
相关论文
共 31 条
[11]  
Hench L. L., 1973, J BIOMED MATER RES S, V4, P25
[12]   BIOCERAMICS - FROM CONCEPT TO CLINIC [J].
HENCH, LL .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1991, 74 (07) :1487-1510
[13]  
JARCHO M, 1981, CLIN ORTHOP RELAT R, V157, P259
[14]  
Jha LJ, 1996, J BIOMED MATER RES, V31, P481, DOI 10.1002/(SICI)1097-4636(199608)31:4<481::AID-JBM7>3.0.CO
[15]  
2-H
[16]  
Kitsugi T, 1996, J BIOMED MATER RES, V32, P149
[17]   BONE BONDING BEHAVIOR OF 3 KINDS OF APATITE CONTAINING GLASS-CERAMICS [J].
KITSUGI, T ;
YAMAMURO, T ;
NAKAMURA, T ;
HIGASHI, S ;
KAKUTANI, Y ;
HYAKUNA, K ;
ITO, S ;
KOKUBO, T ;
TAKAGI, M ;
SHIBUYA, T .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1986, 20 (09) :1295-1307
[18]   BIOACTIVE GLASS-CERAMICS - PROPERTIES AND APPLICATIONS [J].
KOKUBO, T .
BIOMATERIALS, 1991, 12 (02) :155-163
[19]   Spontaneous formation of bonelike apatite layer on chemically treated titanium metals [J].
Kokubo, T ;
Miyaji, F ;
Kim, HM ;
Nakamura, T .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (04) :1127-1129
[20]   SOLUTIONS ABLE TO REPRODUCE INVIVO SURFACE-STRUCTURE CHANGES IN BIOACTIVE GLASS-CERAMIC A-W3 [J].
KOKUBO, T ;
KUSHITANI, H ;
SAKKA, S ;
KITSUGI, T ;
YAMAMURO, T .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1990, 24 (06) :721-734