Multilayer composite ceramic-metal-DLC coatings for sliding wear applications

被引:114
作者
Voevodin, AA [1 ]
Schneider, JM [1 ]
Rebholz, C [1 ]
Matthews, A [1 ]
机构
[1] UNIV HULL,RES CTR SURFACE ENGN,KINGSTON HULL HU6 7RX,N HUMBERSIDE,ENGLAND
基金
英国工程与自然科学研究理事会;
关键词
sliding wear; friction; multilayer coating; composites; diamond-like carbon;
D O I
10.1016/0301-679X(95)00121-J
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The design of anti-friction coatings able to perform well in different wear conditions without lubricants requires a combination of adequate hardness and toughness, good adhesion, a low friction coefficient and a low wear rate. Recently introduced metal-diamond like carbon (DLC) coatings produced by magnetron sputtering of metals from targets, which are to a controlled extent covered with carbon from the chamber atmosphere, can be a step towards the achievement of such a combination. These coatings consist of an amorphous a:CH matrix with the possible incorporation of metal (Ta, W, Nb, Ti), metal carbide and/or graphite grains. Previous studies of TIx%-DLC coatings showed their good protective properties against abrasive, impact and single scratch wear, as well as a requirement for supporting interlayers to successfully apply such coatings to low-cost steels. In the present work an example of the selection of metal-ceramic Ti-TiN-TiCN supporting interlayers is given based on studies of their morphology, structure and mechanical properties. This resulted in the development of Ti-Ti N-TiCN-[TiC-(Ti-x%-DLC)] multilayer composite coatings. Several coatings were prepared with the same supporting interlayer and a variation in the preparation of the Ti-x%-DLC layer. Ball-on-disc experiments were carried out to investigate these coatings in conditions of sliding wear against steel and cemented tungsten carbide balls. CrN, TiN and TiCN coatings were also deposited and tested in the same conditions to provide a reference. Low friction coefficients (below 0.2 at an air humidity of 50% RH) in combination with low normalized wear rates were found for multilayer coatings with upper TI,,,-DLC and Ti-35%-DLC layers. Copyright (C) 1996 Elsevier Science Ltd
引用
收藏
页码:559 / 570
页数:12
相关论文
共 28 条
[11]   DEVELOPMENT AND TESTING OF MULTILAYER PHYSICALLY VAPOR-DEPOSITED COATINGS FOR PISTON RINGS [J].
LYUBIMOV, VV ;
VOEVODIN, AA ;
YEROKHIN, AL ;
TIMOFEEV, YS ;
ARKHIPOV, IK .
SURFACE & COATINGS TECHNOLOGY, 1992, 52 (02) :145-151
[12]   ENGINEERING APPLICATIONS FOR DIAMOND-LIKE CARBON [J].
MATTHEWS, A ;
ESKILDSEN, SS .
DIAMOND AND RELATED MATERIALS, 1994, 3 (4-6) :902-911
[13]   DIFFICULTIES IN ESTIMATING THE RHEOLOGICAL PROPERTIES OF DIAMOND-LIKE FILMS BY MEANS OF NANOINDENTATION TESTS [J].
PIVIN, JC .
THIN SOLID FILMS, 1993, 229 (01) :83-92
[14]   MECHANICAL AND TRIBOLOGICAL PROPERTIES OF DUAL-FREQUENCY PLASMA-DEPOSITED DIAMOND-LIKE CARBON [J].
RAVEH, A ;
MARTINU, L ;
HAWTHORNE, HM ;
WERTHEIMER, MR .
SURFACE & COATINGS TECHNOLOGY, 1993, 58 (01) :45-55
[15]   MECHANICAL-PROPERTIES AND STRUCTURE OF DIAMOND-LIKE CARBON [J].
ROBERTSON, J .
DIAMOND AND RELATED MATERIALS, 1992, 1 (5-6) :397-406
[16]   MICROSTRUCTURAL AND MORPHOLOGICAL EFFECTS ON THE TRIBOLOGICAL PROPERTIES OF ELECTRON ENHANCED MAGNETRON-SPUTTERED HARD COATINGS [J].
SCHNEIDER, JM ;
VOEVODIN, AA ;
REBHOLZ, C ;
MATTHEWS, A .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1995, 13 (04) :2189-2193
[17]   X-RAY-DIFFRACTION INVESTIGATIONS OF MAGNETRON-SPUTTERED TICN COATINGS [J].
SCHNEIDER, JM ;
VOEVODIN, A ;
REBHOLZ, C ;
MATTHEWS, A ;
HOGG, JHC ;
LEWIS, DB ;
IVES, M .
SURFACE & COATINGS TECHNOLOGY, 1995, 74-5 (1-3) :312-319
[18]   REVIEW OF MULTICOMPONENT AND MULTILAYER COATINGS FOR TRIBOLOGICAL APPLICATIONS [J].
SUBRAMANIAN, C ;
STRAFFORD, KN .
WEAR, 1993, 165 (01) :85-95
[19]   INFLUENCE OF APPARATUS GEOMETRY AND DEPOSITION CONDITIONS ON STRUCTURE AND TOPOGRAPHY OF THICK SPUTTERED COATINGS [J].
THORNTON, JA .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY, 1974, 11 (04) :666-670
[20]  
Valli J., 1986, SURF ENG, V2, P49