An in situ FTIR study of galena and pyrite oxidation in aqueous solution

被引:77
作者
Chernyshova, IV [1 ]
机构
[1] St Petersburg State Polytech Univ, St Petersburg 195251, Russia
基金
俄罗斯基础研究基金会;
关键词
galena; pyrite; oxidation; FTIR; ATR; in situ;
D O I
10.1016/S0022-0728(03)00382-6
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
FTIR spectroelectrochemical measurements demonstrated that oxidation of galena starts with the reaction PbS+2xh(+) = Pb1-xS+xPb(2+), which is followed by the reaction PbS + 2h(+) = Pb2+ +S-0. Pb(OH)(2) is formed by the precipitation mechanism. Lead sulfite and thiosulfate and polythionate ions are formed from the elementary sulfur formed in the first oxidation stage. Dissolved oxygen participates in both the cathodic and anodic half-reactions for the galena oxidation. The anodic oxidation of pyrite occurs in two stages. At the first stage, the S deficient clusters or FeS defects degrade by reaction the FeS = Fe2+ +S2-, followed by hydrolysis and (electro)chemical oxidation-precipitation of the products (elemental sulfur, and iron hydroxide). The second stage starts with depopulation of the negatively charged iron acceptor surface states located at the valence band edge. After that, the bulk pyrite oxidation takes place through the thiosulfate pathway. It was shown that the sulfur formed on sulfides has a different origin: on pyrite, sulfur precipitates from solution, while on galena it is residual sulfur left after metal ion leaching from sulfide. The pyrite sulfur is oxidized mainly to polythionates and sulfate, as opposed to galena, for which the main oxysulfur compound is thiosulfate. The sequences of the reactions were explained based on the electronic band structures and correlated with the floatability of the sulfides. A new model of pyrite oxidation at the open circuit potential was suggested, based on the lateral electrochemical inhomogeneity of the pyrite surface. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:83 / 98
页数:16
相关论文
共 98 条
[71]   A VIBRATIONAL SPECTROSCOPIC O-18 TRACER STUDY OF PYRITE OXIDATION [J].
REEDY, BJ ;
BEATTIE, JK ;
LOWSON, RT .
GEOCHIMICA ET COSMOCHIMICA ACTA, 1991, 55 (06) :1609-1614
[72]  
RICHARDSON GM, 1993, J EXPO ANAL ENV EPID, V3, P23
[73]   SEMICONDUCTING CHARACTERISTICS OF GALENA ELECTRODES - RELATIONSHIP TO MINERAL FLOTATION [J].
RICHARDSON, PE ;
ODELL, CS .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1985, 132 (06) :1350-1356
[74]  
RICHARDSON PE, 1992, ELECTROCHEMISTYR MIN, V3
[75]   Kinetics of pyrite formation by the H2S oxidation of iron(II) monosulfide in aqueous solutions between 25 and 125 degrees C: The mechanism [J].
Rickard, D ;
Luther, GW .
GEOCHIMICA ET COSMOCHIMICA ACTA, 1997, 61 (01) :135-147
[76]  
Rosso KM, 1999, AM MINERAL, V84, P1535
[77]   (Bio) chemistry of bacterial leaching - direct vs. indirect bioleaching [J].
Sand, W ;
Gehrke, T ;
Jozsa, PG ;
Schippers, A .
HYDROMETALLURGY, 2001, 59 (2-3) :159-175
[78]   Experimental investigations on iron corrosion products formed in bicarbonate/carbonate containing solutions at 90°C [J].
Savoye, S ;
Legrand, L ;
Sagon, G ;
Lecomte, S ;
Chausse, A ;
Messina, R ;
Toulhoat, P .
CORROSION SCIENCE, 2001, 43 (11) :2049-2064
[79]   Incipient oxidation of fractured pyrite surfaces in air [J].
Schaufuss, AG ;
Nesbitt, HW ;
Kartio, I ;
Laajalehto, K ;
Bancroft, GM ;
Szargan, R .
JOURNAL OF ELECTRON SPECTROSCOPY AND RELATED PHENOMENA, 1998, 96 (1-3) :69-82
[80]   Reactivity of surface chemical states on fractured pyrite [J].
Schaufuss, AG ;
Nesbitt, HW ;
Kartio, I ;
Laajalehto, K ;
Bancroft, GM ;
Szargan, R .
SURFACE SCIENCE, 1998, 411 (03) :321-328