Improvement of straw surface characteristics via thermomechanical and chemical treatments

被引:61
作者
Pan, Mingzhu [1 ,2 ]
Zhou, Dingguo [1 ,2 ]
Zhou, Xiaoyan [1 ,2 ]
Lian, Zhina [3 ]
机构
[1] Nanjing Forestry Univ, Coll Wood Sci & Technol, Nanjing 210037, Jiangsu, Peoples R China
[2] Engn Res Ctr Fast Growing Trees & Agrifibre Mat, Nanjing 210037, Peoples R China
[3] Nanjing Forestry Univ, Minist Educ, Key Lab Forest Genet & Biotechnol, Nanjing 210037, Jiangsu, Peoples R China
关键词
Rice straw; Fibre; Water retention; Xylanase; Hemicellulose hydrolysis; DENSITY FIBERBOARD MDF; MECHANICAL-PROPERTIES; ENZYMATIC-HYDROLYSIS; RICE STRAW; CELLULOSE FIBERS; PARTICLEBOARD; MOISTURE; WATER; HEMICELLULOSES; PRETREATMENT;
D O I
10.1016/j.biortech.2010.05.022
中图分类号
S2 [农业工程];
学科分类号
0828 ;
摘要
This study focused on effects of thermomechanical treatment, acid hydrolysis and enzymatic hydrolysis of rice straw fibre on its water resistant. Xylose and arabinose yields were 19.97% and 2.55%, respectively with thermomechanical treatment, 24.35% and 3.18% with acid hydrolysis, and 20.11% and 2.73% with enzymatic hydrolysis. The acid treatment dissolved hemicellulose significantly, leading to more fines and more voids in the surface of the rice straw fibre. The fines showed a higher water retention value (WRV) of 137.41% and exhibited higher swelling capacity. An increase in acid loading resulted in the increased WRV. The enzymatic hydrolysis increased the crystallinity of cellulose, but no significant correlation could be found between the chemical component and the water resistance of the rice straw fibre. (c) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:7930 / 7934
页数:5
相关论文
共 37 条
[1]   Effect of silica content on rice straw ruminal degradation [J].
Agbagla-Dohnani, A ;
Nozière, P ;
Gaillard-Martinie, B ;
Puard, M ;
Doreau, M .
JOURNAL OF AGRICULTURAL SCIENCE, 2003, 140 :183-192
[2]   Water-based woody biorefinery [J].
Amidon, Thomas E. ;
Liu, Shijie .
BIOTECHNOLOGY ADVANCES, 2009, 27 (05) :542-550
[3]  
[Anonymous], 1996, D110796 ASTM INT
[4]  
[Anonymous], 1991, Tappi Useful Methods, P54
[5]  
[Anonymous], 2005, HDB WOOD CHEM WOOD C, DOI [DOI 10.1201/B12487, 10.1201/b12487]
[6]   Enzymatic hydrolysis of dissolved corn stalk hemicelluloses: reaction kinetics and modeling [J].
Belkacemi, K ;
Hamoudi, S .
JOURNAL OF CHEMICAL TECHNOLOGY AND BIOTECHNOLOGY, 2003, 78 (07) :802-808
[7]  
Boonstra MJ, 2006, HOLZ ROH WERKST, V64, P157, DOI 10.1007/s00107-005-0055-y
[8]  
Dashek W.V., 1997, Methods in plant biochemistry and molecular biology
[9]   Fractionation and molecular characteristics of cellulose during enzymatic hydrolysis [J].
Eremeeva, T ;
Bikova, T ;
Eisimonte, M ;
Viesturs, U ;
Treimanis, A .
CELLULOSE, 2001, 8 (01) :69-79
[10]   Dimensional stability of MDF panels produced from fibres treated with maleated polypropylene wax [J].
Garcia, RA ;
Cloutier, A ;
Riedl, B .
WOOD SCIENCE AND TECHNOLOGY, 2005, 39 (08) :630-650