Piezoelectric and Dielectric Properties of Lead-Free (1-x)(Bi0.5K0.5)TiO3-xBiFeO3 Ceramics

被引:31
作者
Kim, J. M. [1 ]
Sung, Y. S. [1 ]
Cho, J. H. [1 ]
Song, T. K. [1 ]
Kim, M. H. [1 ]
Chong, H. H. [2 ]
Park, T. G. [2 ]
Do, D. [3 ]
Kim, S. S. [3 ]
机构
[1] Changwon Natl Univ, Sch Nano & Adv Mat Engn, Gyeongnam 641773, South Korea
[2] Changwon Natl Univ, Dept Elect Engn, Gyeongnam 641773, South Korea
[3] Changwon Natl Univ, Dept Phys, Gyeongnam 641773, South Korea
关键词
Lead-free; bismuth potassium titanate; bismuth ferrite; depolarization temperature; K0.5BI0.5TIO3;
D O I
10.1080/00150193.2010.482448
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Dielectric and piezoelectric properties of lead-free (1-x)(Bi0.5K0.5)TiO3-xBiFeO(3) ceramics prepared by a conventional solid-state reaction method were studied in the range of x = 0 similar to 40 mol%. A tetragonal perovskite structure was maintained at x = 0 similar to 10 mol% forming a solid solution between (Bi0.5K0.5)TiO3 and BiFeO3 with no secondary phase. Piezoelectric coefficient (d(33)) increased from 31 pC/N at x = 0 mol% to 64 pC/N at x = 6 mol% and then decreased with further addition of x. Depolarization temperature (T-d) gradually decreased with increasing x from 302 degrees C at x = 0 mol% to 163 degrees C at x = 20 mol% and slightly increased up 180 degrees C at x = 40 mol%.
引用
收藏
页码:88 / 92
页数:5
相关论文
共 11 条
[1]   Ferroelectric and leakage current behaviors of BiFeO3-Bi(Zn1/2Ti1/2)O3 ceramics [J].
Cho, J. H. ;
Song, T. K. ;
Wang, L. ;
Yeo, H. -G. ;
Sung, Y. -S. ;
Kim, M. -H. ;
Park, D. -S. .
JOURNAL OF APPLIED PHYSICS, 2009, 105 (06)
[2]   Ferroelectric and piezoelectric properties of (Bi1/2K1/2)TiO3 ceramics fabricated by hot-pressing method [J].
Hiruma, Yuji ;
Marumo, Kota ;
Aoyagi, Rintaro ;
Nagata, Hajime ;
Takenaka, Tadashi .
JOURNAL OF ELECTROCERAMICS, 2008, 21 (1-4) :296-299
[3]   Depolarization temperature and piezoelectric properties of (Bi1/2Na1/2)TiO3-(Bi1/2Li1/2)TiO3-(Bi1/2K1/2)TiO3 lead-free piezoelectric ceramics [J].
Hiruma, Yuji ;
Nagata, Hajime ;
Takenaka, Tadashi .
CERAMICS INTERNATIONAL, 2009, 35 (01) :117-120
[4]   Ferroelectric Na0.5Bi0.5TiO3 and K0.5Bi0.5TiO3 perovskites and their solid solutions [J].
Isupov, VA .
FERROELECTRICS, 2005, 315 :123-147
[5]  
Jaffe B., 1971, Piezoelectric Ceramics, P136
[6]   Microstructures and piezoelectric properties in the Li2O-Excess 0.95(Na0.5K0.5)NbO3-0.05LiTaO3 ceramics [J].
Kim, Min-Soo ;
Jeong, Soon-Jong ;
Song, Jae-Sung .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2007, 90 (10) :3338-3340
[7]   Electromechanical and dielectric properties of Na0.5Bi0.5TiO3-K0.5Bi0.5TiO3-BaTiO3 [J].
Li, YM ;
Chen, W ;
Xu, Q ;
Zhou, J ;
Gu, XY ;
Fang, SQ .
MATERIALS CHEMISTRY AND PHYSICS, 2005, 94 (2-3) :328-332
[8]   Dielectric relaxor properties of K0.5Bi0.5TiO3 ferroelectrics prepared by sol-gel method [J].
Li, ZF ;
Wang, CL ;
Zhong, WL ;
Li, JC ;
Zhao, ML .
JOURNAL OF APPLIED PHYSICS, 2003, 94 (04) :2548-2552
[9]   Electrical properties of K0.5Bi0.5TiO3 [J].
Rao, P. Vijaya Bhaskar ;
Ramana, E. V. ;
Sankaram, T. Bhima .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 467 (1-2) :293-298
[10]   Enhanced piezoelectric properties of (Bi0.5K0.5+xLiy)TiO3 ceramics by K nonstoichiometry and Li addition [J].
Sung, Y. S. ;
Lee, H. M. ;
Du, W. ;
Yeo, H. G. ;
Lee, S. C. ;
Cho, J. H. ;
Song, T. K. ;
Kim, M. H. .
APPLIED PHYSICS LETTERS, 2009, 94 (06)