Polyurethanes with monodisperse rigid segments based on a diamine-diamide chain extender

被引:24
作者
Biemond, G. J. E. [1 ,2 ]
Braspenning, K. [1 ]
Gaymans, R. J. [1 ]
机构
[1] Univ Twente, Dept Sci & Technol, NL-7500 AE Enschede, Netherlands
[2] Dutch Polymer Inst, NL-5600 AX Eindhoven, Netherlands
关键词
polyurethane; monodisperse; amide; properties; segmented block copolymer;
D O I
10.1002/app.27282
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Polyether(bisurethane-bisurea-bisamide)s (PEUUA) based on poly(tetramethylene oxide) (PTMO) were synthesized by chain extension of PTMO endcapped with a diisocyanate (DI), and a diamine-diamide extender. The prepolymers were PTMOs with molecular weights between 1270 and 2200 g mol(-1), either endcapped with 4,4 '-diphenylmethane diisocyanate (MDI), 2,4-toluene diisocyanate (2,4-TDI), or 1,6-hexane diisocyante (HDI) and with a low content of free diisocyanate (< 0.1 wt %). The diamine-diamide (6A6) extender was based on hexamethylene diamine (6) and adipic acid (A). In this way, segmented polyurethanes with monodisperse rigid segments (DI-6A6-DI) were obtained. The PEUUAs were characterized by DSC as well as temperature-dependent FTIR and DMTA. The mechanical properties of the polymers were evaluated by compression set and tensile test measurements. The polyurethanes with monodisperse rigid segments displayed low glass transition temperatures, almost temperature-independent rubbery plateaus and sharp melting temperatures. The crystallinities of the hard segments were 70-80% upon heating and 40-60% upon cooling. The rate of crystallization was moderately fast as the supercooling (T-m - T-c) was in the order 36-54 degrees C. The polyurethanes based on HDI had a much higher rubber modulus as compared to the MDI and 2,4-TDI-based polymers, because of a higher degree of crystallinity and/or a higher aspect ratio of the crystallites. The HDI residues are flexible and not sterically hindered and could therefore be more easily packed than MDI or 2,4-TDI residues. Polyurethanes with monodisperse DI-6A6-DI hard segments have interesting properties. (c) 2007 Wiley Periodicals, Inc.
引用
收藏
页码:2180 / 2189
页数:10
相关论文
共 28 条
[21]   Tensile and elastic properties of segmented copolyetheresteramides with uniform aramid units [J].
Niesten, MCEJ ;
Gaymans, RJ .
POLYMER, 2001, 42 (14) :6199-6207
[22]  
Socretes G., 2001, Infrared Characteristic Group Frequencies
[23]  
Szycher M., 2013, Szycher's Handbook of Polyurethanes
[24]   Polyurethane elastomers with amide chain extenders of uniform length [J].
van der Schuur, M ;
Noordover, B ;
Gaymans, RJ .
POLYMER, 2006, 47 (04) :1091-1100
[25]   Structure-property relations of poly(propylene oxide) block copolymers with monodisperse and polydisperse crystallisable segments [J].
van der Schuur, M ;
de Boer, J ;
Gaymans, RJ .
POLYMER, 2005, 46 (22) :9243-9256
[26]   Structure-property relations of segmented block copolymers with liquid-liquid demixed morphologies [J].
van der Schuur, M ;
van der Heide, E ;
Feijen, J ;
Gaymans, RJ .
POLYMER, 2005, 46 (11) :3616-3627
[27]   Segmented block copolymers based on poly(propylene oxide) and monodisperse polyamide-6,T segments [J].
Van der Schuur, Martijn ;
Gaymans, Reinoud J. .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 2006, 44 (16) :4769-4781
[28]   Properties and morphology of segmented copoly(ether urea)s with uniform hard segments [J].
Versteegen, RM ;
Kleppinger, R ;
Sijbesma, RP ;
Meijer, EW .
MACROMOLECULES, 2006, 39 (02) :772-783