Enhanced internal oxidation as trigger for breakaway oxidation of Fe-Cr alloys in gases containing water vapor

被引:148
作者
Essuman, E.
Meier, G. H.
Zurek, J. [1 ]
Haensel, M.
Singheiser, L.
Quadakkers, W. J.
机构
[1] Forschungszentrum Julich, IEF 2, D-52428 Julich, Germany
[2] Univ Pittsburgh, Pittsburgh, PA USA
关键词
chromia; iron alloys; hydrogen; oxidation;
D O I
10.1016/j.scriptamat.2007.06.058
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Binary Fe-Cr alloys were studied with respect to isothermal oxidation behavior at 900 degrees C in Ar-O-2, Ar-H2O and Ar-H-2-H2O gas mixtures. Chromium in solution exhibits a higher tendency to become internally oxidized in the gases containing water vapor than in the Ar-O-2 gas because of hydrogen dissolution in the alloy. This mechanism explains why Fe-Cr alloys with intermediate Cr contents (e.g., 10-20 wt.%) exhibit protective chromia-rich scale formation in dry gases but tend to form breakaway-type Fe-rich oxides in wet gases. (C) 2007 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:845 / 848
页数:4
相关论文
共 19 条
[11]   Effect of water vapour on growth and adherence of chromia scales formed on Cr in high and low PO2-environments at 1000 and 1050°C [J].
Michalik, M. ;
Haensel, M. ;
Zurek, J. ;
Singheiser, L. ;
Quadakkers, W. J. .
MATERIALS AT HIGH TEMPERATURES, 2005, 22 (3-4) :213-221
[12]   Corrosion behavior of ferritic steels on the air sides of boiler tubes in a steam/air dual environment [J].
Nakagawa, K ;
Matsunaga, Y ;
Yanagisawa, T .
MATERIALS AT HIGH TEMPERATURES, 2003, 20 (01) :67-73
[13]  
Rahmel A., 1965, Corrosion Science, V5, P333, DOI DOI 10.1016/S0010-938X(65)90500-7
[14]   Parameters determining the breakaway oxidation behaviour of ferritic martensitic 9%Cr steels in environments containing H2O [J].
Schütze, M ;
Renusch, D ;
Schorr, M .
CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2004, 39 (02) :157-166
[15]  
Thiele M, 1997, VGB KRAFTWERKSTECHN, V77, P135
[16]   Formation and disappearance of an internal oxidation zone in the initial stage of the steam oxidation of Fe-9Cr-0.26Si ferritid-steel [J].
Ueda, M ;
Nanko, M ;
Kawamura, K ;
Maruyama, T .
MATERIALS AT HIGH TEMPERATURES, 2003, 20 (02) :109-114
[17]  
YANG Z, 2003, SOLID STATE LETT, V6, pB35
[18]   Anomalous temperature dependence of oxidation kinetics during steam oxidation of ferritic steels in the temperature range 550-650°C [J].
Zurek, J ;
Wessel, E ;
Niewolak, L ;
Schmitz, F ;
Kern, TU ;
Singheiser, L ;
Quadakkers, WJ .
CORROSION SCIENCE, 2004, 46 (09) :2301-2317
[19]  
ZUREK J, IN PRESS MAT SCI E A