Sol-gel prepared active ternary oxide coating on titanium in cathodic protection

被引:21
作者
Panic, Vladimir V. [1 ]
Nikolic, Branislav Z. [2 ]
机构
[1] ICTM, Ctr Electrochem, Belgrade 11000, Serbia
[2] Univ Belgrade, Fac Technol & Met, Belgrade 11000, Serbia
关键词
ruthenium-oxide-based coatings; sol-gel procedure; iridium oxide; cathodic protection; stability;
D O I
10.2298/JSC0712393P
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The characteristics of a ternary oxide coating, on titanium, which consisted of TiO2, RuO2 and IrO2 in the molar ratio 0.6:0.3:0.1, calculated on the metal atom, were investigated for potential application for cathodic protection in a seawater environment. The oxide coatings on titanium were prepared by the sol-gel procedure from a mixture of inorganic oxide sols, which were obtained by forced hydrolysis of metal chlorides. The morphology of the coating was examined by scanning electron microscopy. The electrochemical properties of activated titanium anodes were investigated by cyclic voltammetry and polarization measurements in a H2SO4- and NaCl-containing electrolyte, as well as in seawater sampled on the Adriatic coast in Tivat, Montenegro. The anode stability during operation in seawater was investigated by the galvanostatic accelerated corrosion stability test. The morphology and electrochemical characteristics of the ternary coating are compared to that of a sol-gel-prepared binary Ti0.6Ru0.40O2 coating. The activity of the ternary coating was similar to that of the binary Ti0.6Ru0.4O2 coating in the investigated solutions. However, the stability in seawater is found to be considerably greater for the ternary coating.
引用
收藏
页码:1393 / 1402
页数:10
相关论文
共 35 条
[1]   Effect of warship impressed current cathodic protection configuration on low frequency current output modulations associated with propeller/shaft rotation [J].
Akomah, AO ;
Dahele, JS ;
Tighe-Ford, DJ .
BRITISH CORROSION JOURNAL, 2002, 37 (02) :114-116
[2]   Interfacial properties of oxides with technological impact in electrochemistry [J].
Ardizzone, S ;
Trasatti, S .
ADVANCES IN COLLOID AND INTERFACE SCIENCE, 1996, 64 :173-251
[3]   WEAR MECHANISMS OF ANODES [J].
BECK, F .
ELECTROCHIMICA ACTA, 1989, 34 (06) :811-822
[4]  
Cai T.-X., 2006, CORR POTECTION, V27, P522
[5]   Kinetics of oxygen reduction at RuO2-coated titanium electrode in alkaline solution [J].
Chang, CC ;
Wen, TC .
JOURNAL OF APPLIED ELECTROCHEMISTRY, 1997, 27 (03) :355-363
[6]  
Conway B. E., 1999, ELECTROCHEMICAL SUPE
[7]  
Cornell A., 2004, P 4 K SCHWAB CORR S, P326
[8]   Evaluation of the effect of ruthenium oxide on the properties of composite electrodes used in cathodic protection [J].
Darowicki, K ;
Janicki, S .
CORROSION SCIENCE, 1999, 41 (06) :1165-1173
[9]   Reasons for the DSA passivation during chlorate electrolysis and the means for extending the anode service life [J].
Eberil', VI ;
Novikov, EA ;
Mazanko, AF .
RUSSIAN JOURNAL OF ELECTROCHEMISTRY, 2001, 37 (10) :1054-1058
[10]   New concept for cathodic protection of offshore pipelines to reduce hydrogen induced stress cracking (HISC) in high strength 13%Cr stainless steels [J].
Eliassen, S .
CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2004, 39 (01) :31-37