Role of intermetallic phases in localized corrosion of AA5083

被引:325
作者
Yasakau, Kiryl A.
Zheludkevich, Mikhail L. [1 ]
Lamaka, Sviatlana V.
Ferreira, Mario G. S.
机构
[1] Univ Aveiro, CICECO, Dept Ceram & Glass Engn, P-3810 Aveiro, Portugal
[2] Inst Super Tecn, ICEMS, Dept Chem Engn, P-1049 Lisbon, Portugal
关键词
AA5083; corrosion; pitting; scanning Kelvin probe force microscopy; intermetallic phases;
D O I
10.1016/j.electacta.2006.12.072
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The presence of intermetallic inclusions very often plays a crucial role for the susceptibility of different aluminium alloys to localized corrosion attack. The intimate details of localized corrosion of 5083 aluminium alloy have been studied in the present work. Local techniques such as scanning Kelvin probe force microscopy, in situ atomic force microscopy, scanning electron microscopy coupled with energy dispersive spectroscopy were used to investigate the mechanisms and the kinetics of localized corrosion attack. The importance of iron-rich and Mg2Si intermetallic phases in the initiation of corrosion processes is demonstrated in the paper. The Mg2Si phase has a potential lower relatively to the matrix. Moreover, the high reactivity of magnesium leads to the dissolution and consequently to the fast dealloying of these intermetallics. However, hydroxide (Mg(OH)(2) and SiO2 center dot nH(2)O) deposits formed during corrosion act as an additional diffusion barrier hindering the deep propagation of pits. The iron containing intermetallics have the potential higher with respect to the aluminum matrix playing the role of effective cathodic centers for oxygen reduction causing anodic polarization and pitting in the surrounding alloy matrix. Dealloying of such intermetallics with subsequent iron enrichment was also revealed. Pitting initiation seems to be statistical and independent of the composition of Fe-rich intermetallics. However, the active growth of the pits prevents initiation of localized corrosion attack in nearby sites. A new pit can start to grow only when a neighbor one becomes passivated. (c) 2007 Elsevier Ltd. All rights reserved.
引用
收藏
页码:7651 / 7659
页数:9
相关论文
共 26 条
[1]   Effect of solution heat treatment on galvanic coupling between intermetallics and matrix in AA7075-T6 [J].
Andreatta, F ;
Terryn, H ;
de Wit, JHW .
CORROSION SCIENCE, 2003, 45 (08) :1733-1746
[2]   Inhibition of 5083 aluminium alloy and galvanised steel by lanthanide salts [J].
Arenas, MA ;
Bethencourt, M ;
Botana, FJ ;
de Damborenea, J ;
Marcos, M .
CORROSION SCIENCE, 2001, 43 (01) :157-170
[3]   Emulation and study of the corrosion behavior of Al alloy 2024-T3 using a wire beam electrode (WBE) in conjunction with scanning vibrating electrode technique (SVET) [J].
Battocchi, D ;
He, J ;
Bierwagen, GP ;
Tallman, DE .
CORROSION SCIENCE, 2005, 47 (05) :1165-1176
[4]   Effects of Zn additions on the grain boundary precipitation and corrosion of Al-5083 [J].
Carroll, MC ;
Gouma, PI ;
Mills, MJ ;
Daehn, GS ;
Dunbar, BR .
SCRIPTA MATERIALIA, 2000, 42 (04) :335-340
[5]   Effects of minor Cu additions on a Zn-modified Al-5083 alloy [J].
Carroll, MC ;
Gouma, PI ;
Daehn, GS ;
Mills, MJ .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 319 :425-428
[6]   Low-cycle fatigue of friction stir welded Al-Mg alloys [J].
Czechowski, A .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2005, 164 :1001-1006
[7]  
Dean J.A., 2001, Lange's Handbook of Chemistry, V15
[8]  
Dupuy L, 2002, ACTA MATER, V50, P3251, DOI 10.1016/S1359-6454(02)00147-7
[9]   CORROSION OF 5456-H117 ALUMINUM IN HIGH-VELOCITY SEA-WATER [J].
GEHRING, GA ;
PETERSON, MH .
CORROSION, 1981, 37 (04) :232-242
[10]   Characterization of corrosion interfaces by the scanning Kelvin probe force microscopy technique [J].
Guillaumin, V ;
Schmutz, P ;
Frankel, GS .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2001, 148 (05) :B163-B173