摘要
Hard-chrome plate is traditionally employed as a wear resistant surface. However, concerns that the processing of such materials is not environmentally friendly have lead to a search for potential replacements. This work examines the behaviour of two alloy systems, namely Co-W and Co-W-Fe. Alloys from these systems were electrodeposited onto steel substrates. The Co-W alloys were further heat treated to increase their hardness, although this was deemed unnecessary for the Co-W-Fe alloys which had high as-deposited hardnesses. The sliding wear behaviour of these materials was examined, along with the behaviour of a hard chrome under similar conditions. It was found that under some conditions, the Co-W alloys exhibited a wear resistance and a coefficient of friction similar to that of hard chrome. Moreover, the corrosion resistance of the Co-W alloys was higher than that of the hard-chrome plate. The Co-W-Fe alloys exhibited a high as-deposited hardness. At a critical iron level of 30 wt.%, the wear rate of these coatings decreased substantially. All the Co-W-Fe coatings were more corrosion resistant than the hard chrome; however, even the most wear resistant exhibited a high coefficient of friction and more wear than the hard chrome. (C) 2003 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:917 / 923
页数:7
相关论文
共 22 条
[1]   MICROSTRUCTURE OF ELECTRODEPOSITED CO-W THIN-FILMS [J].
ADMON, U ;
DARIEL, MP ;
GRUNBAUM, E .
JOURNAL OF APPLIED PHYSICS, 1986, 59 (06) :2002-2009
[2]  
CAPEL H, IN PRESS
[3]  
CAPEL H, 2002, P AESF SUR FIN 2002, P123
[4]   Corrosion and wear properties of electrodeposited amorphous chrome [J].
Choi, Y .
JOURNAL OF MATERIALS SCIENCE, 1997, 32 (06) :1581-1586
[5]  
ElSharif M, 1997, T I MET FINISH, V75, pB143
[6]  
Eskin S, 1998, PLAT SURF FINISH, V85, P79
[7]   CRYSTALLIZATION OF SINGLE-LAYERED AND MULTILAYERED AMORPHOUS CO-W FILMS [J].
FEDOSYUK, VM ;
RIVEIRO, JM .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1992, 143 (2-3) :153-156
[8]  
Gangmin C., 2001, T IMF, V79, P81
[9]  
Ibrahim S.K., 1998, T IMF, V76, P161
[10]   Wear characteristics of electrolytic hard chrome and thermal sprayed WC-10Co-4Crcoatings sliding against Al-Ni-bronze in air at 21 °C and at-40 °C [J].
Ko, PL ;
Robertson, MF .
WEAR, 2002, 252 (11-12) :880-893