Effect of humidity on the ordering of PEO-based copolymer thin films

被引:102
作者
Bang, Joona
Kim, Bumjoon J.
Stein, Gila E.
Russell, Thomas P.
Li, Xuefa
Wang, Jin
Kramer, Edward J. [1 ]
Hawker, Craig J.
机构
[1] Korea Univ, Dept Chem & Biol Chem Engn, Seoul 136701, South Korea
[2] Univ Calif Santa Barbara, Mat Res Lab, Santa Barbara, CA 93106 USA
[3] Univ Calif Santa Barbara, Dept Mat, Santa Barbara, CA 93106 USA
[4] Univ Calif Santa Barbara, Dept Chem Engn, Santa Barbara, CA 93106 USA
[5] Univ Calif Santa Barbara, Dept Chem & Biochem, Santa Barbara, CA 93106 USA
[6] Univ Massachusetts, Dept Polymer Sci & Engn, Amherst, MA 01003 USA
[7] Argonne Natl Lab, Adv Photon Source, Argonne, IL 60439 USA
关键词
D O I
10.1021/ma0710737
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Solvent cast diblock and triblock copolymer films of poly(ethylene oxide-b-styrene) (PEO-b-PS) and poly(ethylene oxide-b-methyl meth acrylate-b-styrene) (PEO-b-PMMA-b-PS), with cylindrical microdomains of PEO or PMMA-PEO, have a high degree of lateral ordering after solvent annealing. The relative humidity of the vapor during the solvent annealing has been shown to play an important role in achieving this order. After solvent annealing under high humidity a PEO-b-PMMA-b-PS triblock copolymer having a lamellar morphology in bulk develops a hexagonal array of depressed PEO domains on the film surface while the film surface remains flat under less humid conditions. Cross-sectional TEM and GISAXS show that the film annealed under high humidity conditions exhibits a well-defined hexagonally perforated lamellar (HPL) structure throughout its thickness, whereas a stack of lamellae aligned parallel to the surface is evident for films annealed at lower humidity. These results demonstrate the switchable nanoscopic structure of these films and strongly suggest that water vapor induces the morphological transition from lamellar to HPL by swelling the PEO domains.
引用
收藏
页码:7019 / 7025
页数:7
相关论文
共 57 条
[1]   Structure of shear-induced perforated layer phase in styrene-isoprene diblock copolymer melts [J].
Ahn, JH ;
Zin, WC .
MACROMOLECULES, 2000, 33 (02) :641-644
[2]   Nanofabrication of integrated magnetoelectronic devices using patterned self-assembled copolymer templates [J].
Bal, M ;
Ursache, A ;
Tuominen, MT ;
Goldbach, JT ;
Russell, TP .
APPLIED PHYSICS LETTERS, 2002, 81 (18) :3479-3481
[3]   Defect-free nanoporous thin films from ABC triblock copolymers [J].
Bang, Joona ;
Kim, Seung Hyun ;
Drockenmuller, Eric ;
Misner, Matthew J. ;
Russell, Thomas P. ;
Hawker, Craig J. .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2006, 128 (23) :7622-7629
[4]   BLOCK COPOLYMER THERMODYNAMICS - THEORY AND EXPERIMENT [J].
BATES, FS ;
FREDRICKSON, GH .
ANNUAL REVIEW OF PHYSICAL CHEMISTRY, 1990, 41 (01) :525-557
[5]   Integration of self-assembled diblock copolymers for semiconductor capacitor fabrication [J].
Black, CT ;
Guarini, KW ;
Milkove, KR ;
Baker, SM ;
Russell, TP ;
Tuominen, MT .
APPLIED PHYSICS LETTERS, 2001, 79 (03) :409-411
[6]   Hierarchical nanoparticle assemblies formed by decorating breath figures [J].
Böker, A ;
Lin, Y ;
Chiapperini, K ;
Horowitz, R ;
Thompson, M ;
Carreon, V ;
Xu, T ;
Abetz, C ;
Skaff, H ;
Dinsmore, AD ;
Emrick, T ;
Russell, TP .
NATURE MATERIALS, 2004, 3 (05) :302-306
[7]   Entropy difference between crystal phases [J].
Bolhuis, PG ;
Frenkel, D ;
Mau, SC ;
Huse, DA .
NATURE, 1997, 388 (6639) :235-236
[8]   Cylindrical morphologies in asymmetric ABC triblock copolymers [J].
Breiner, U ;
Krappe, U ;
Abetz, V ;
Stadler, R .
MACROMOLECULAR CHEMISTRY AND PHYSICS, 1997, 198 (04) :1051-1083
[9]   Structural characterization of the "knitting pattern" in polystyrene-block-poly(ethylene-co-butylene)-block-poly(methylmethacrylate) triblock copolymers [J].
Breiner, U ;
Krappe, U ;
Thomas, EL ;
Stadler, R .
MACROMOLECULES, 1998, 31 (01) :135-141
[10]   Free energy of crystalline solids: A lattice-switch Monte Carlo method [J].
Bruce, AD ;
Wilding, NB ;
Ackland, GJ .
PHYSICAL REVIEW LETTERS, 1997, 79 (16) :3002-3005