Moisture resistance of the low-emissivity coatings with a layer structure of Al-doped ZnO/Ag/Al-doped ZnO

被引:103
作者
Ando, E [1 ]
Miyazaki, M [1 ]
机构
[1] Asahi Glass Co Ltd, Res Ctr, Kanagawa Ku, Yokohama, Kanagawa 2218755, Japan
关键词
coatings; silver; sputtering; zinc oxide;
D O I
10.1016/S0040-6090(01)01045-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The moisture durability of sputtered low-emissivity (low-e) coatings with a single silver layer structure of ZnO/Ag/ZnO/glass and Al-doped ZnO/Ag/Al-doped ZnO/glass was investigated. Zinc oxide and aluminum-doped zinc oxide (AZO) films were reactively deposited from pure Zn, 99Zn-1Al, 97Zn-3Al, 95Zn-5Al, 90Zn-10Al (at.%) targets. The aluminum content in the AZO films was measured by secondary ion mass spectroscopy (SIMS). The deposition rate and internal stress of the AZO films were measured. After a moisture durability test at 50 degreesC in 95% relative humidity for 12 days, the coatings were analyzed using optical microscopy, X-ray diffraction (XRD) and scanning electron microscopy (SEM). It was observed that the Al addition reduced the internal stress of the oxide films, and the AZO/Ag/AZO coatings had a better moisture resistance. However, the Al addition led to a decreased deposition rate of the oxide films, and the addition of excess Al resulted in a different moisture degradation with a hazy appearance that might be due to an undesirable hydrate formation in the low-e coating. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:289 / 293
页数:5
相关论文
共 7 条
[1]   Moisture degradation mechanism of silver-based low-emissivity coatings [J].
Ando, E ;
Miyazaki, M .
THIN SOLID FILMS, 1999, 351 (1-2) :308-312
[2]   Sputtered tin silicon oxide films for durable solar control coatings [J].
Ando, E ;
Suzuki, S ;
Shimizu, J ;
Hayashi, Y .
THIN SOLID FILMS, 1999, 351 (1-2) :301-307
[3]   Sputtered silver-based low-emissivity coatings with high moisture durability [J].
Ando, E ;
Suzuki, S ;
Aomine, N ;
Miyazaki, M ;
Tada, M .
VACUUM, 2000, 59 (2-3) :792-799
[4]  
ARBAB M, 1997, PPG TECHNOL J, V3, P29
[5]   DURABILITY IMPROVEMENT OF AG-BASED LOW-EMISSIVITY COATINGS [J].
MIYAZAKI, M ;
ANDO, E .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1994, 178 (pt 2) :245-249
[6]   DURABILITY OF AG BASED LOW-EMISSIVITY COATINGS [J].
NADEL, SJ .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1987, 5 (04) :2709-2713
[7]   OBSERVATIONS ON HUMIDITY-INDUCED DEGRADATION OF AG-BASED LOW-EMISSIVITY FILMS [J].
ROSS, RC .