Diameter dependence of Raman intensities for single-wall carbon nanotubes -: art. no. 153401

被引:47
作者
Alvarez, L [1 ]
Righi, A
Rols, S
Anglaret, E
Sauvajol, JL
Muñoz, E
Maser, WK
Benito, AM
Martínez, MT
de la Fuente, GF
机构
[1] Univ Montpellier 2, Dynam Phases Condensees Grp, CNRS, UMR 5581, F-34095 Montpellier 5, France
[2] CSIC, Inst Carboquim, Zaragoza 50015, Spain
[3] Univ Zaragoza, CSIC, ICMA, Zaragoza 50015, Spain
[4] Inst Max Von Laue Paul Langevin, F-38042 Grenoble, France
来源
PHYSICAL REVIEW B | 2001年 / 63卷 / 15期
关键词
D O I
10.1103/PhysRevB.63.153401
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The Raman-active radial breathing modes (RBM) and tangential modes (TM) of single wall carbon nanotubes (SWNT) are studied at fixed laser excitation energy 2.41 eV (514.5 nm). We focus on the striking diameter dependence of the relative intensity of the TM and RBM between 0.9 and 2.1 nm, which displays a series of plateaux separated by well-defined minima around 1.35 and 0.9 nm. This relates to the diameter dependence of allowed optical transitions (AOT) in SWNT. Diameters in the range 1-1.3 nm (above 1.4 nm) correspond to metallic (semiconducting) SWNT in resonance at 2.41 eV. The minima correspond to out-of-resonance conditions for TM. The measurement of the diameter dependence of the TM intensity for fixed laser energies is an alternative experimental way to plot the envelopes of the domains of AOT in SWNT.
引用
收藏
页数:4
相关论文
共 21 条
  • [21] Crystalline ropes of metallic carbon nanotubes
    Thess, A
    Lee, R
    Nikolaev, P
    Dai, HJ
    Petit, P
    Robert, J
    Xu, CH
    Lee, YH
    Kim, SG
    Rinzler, AG
    Colbert, DT
    Scuseria, GE
    Tomanek, D
    Fischer, JE
    Smalley, RE
    [J]. SCIENCE, 1996, 273 (5274) : 483 - 487