spinel;
Al-doped spinel;
cycleability;
the intensity ratio of (311)/(400) peaks;
lithium battery;
D O I:
10.1016/S0378-7753(00)00652-2
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
LiAlxMn2-xO4 has been synthesized using various aluminum starting materials, such as Al(NO3)(3), Al(OH)(3). AlF3 and Al2O3 at 600-800 degreesC for 20 h in air or oxygen atmosphere. A melt-impregnation method was used to synthesize Al-doped spinel with good battery performance in this research. The Al-doped content and the intensity ratio of (3 1 1)/(4 0 0) peaks can be important parameters in synthesizing Al-doped spinel which satisfies the requirements of high discharge capacity and good cycleability at the same time, The decrease in Mn3+ ion by Al substitution induces a high average oxidation state of Mn ion in the LiAlxMn2-xO4 material. The electrochemical behavior of all samples was studied in Li/LiPF6-EC/DMC (1:2 by volume)/LiAlxMn2-xO4 cells. Especially, the initial and last discharge capacity of LiAl0.09Mn1.97O4 using LiOH, Mn3O4 and Al(OH)(3) complex were 128.7 and 115.5 mAh/g after 100 cycles. The Al substitution in LiMn2O4 was an excellent method of enhancing the cycleability of stoichiometric spinel during electrochemical cycling. (C) 2001 Elsevier Science B.V. All rights reserved.