Porous silicon negative electrodes for rechargeable lithium batteries

被引:149
作者
Shin, HC
Corno, JA
Gole, JL
Liu, ML [1 ]
机构
[1] Sch Mat Sci & Engn, Atlanta, GA 30332 USA
[2] Georgia Inst Technol, Sch Phys, Atlanta, GA 30332 USA
关键词
porous silicon; porous structure; etching; lithium battery;
D O I
10.1016/j.jpowsour.2004.06.073
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Porous silicon (PS) negative electrodes with one-dimensional (1-D) channels have been successfully fabricated using an electrochemical etching process. The peak current and the amount of charge transferred during cyclic voltametry (CV) increase with the channel depth of the PS, indicating that the channel wall of the PS participates in the lithiation/delithiation process. The channel structure of the PS electrodes remains essentially the same after 35 CV cycles in spite of the severe deformation of the channel wall during the repetitive lithium alloying/dealloying process. The specific capacity of the PS depends critically on the degree of activation of the PS before the galvanostatic charge/discharge experiment. For an exemplary PS electrode pre-activated by 20 CV cycles, the reversible specific capacity of the PS reached 43 muA h cm(-2). After a subsequent activation by 10 CV cycles, the capacity increased by 40% (60 muA h cm(-2)). One-dimensional porous silicon appears to be a promising negative electrode for rechargeable micro-batteries. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:314 / 320
页数:7
相关论文
共 17 条
  • [1] MULTINARY ALLOY ELECTRODES FOR SOLID-STATE BATTERIES .1. A PHASE-DIAGRAM APPROACH FOR THE SELECTION AND STORAGE PROPERTIES DETERMINATION OF CANDIDATE ELECTRODE MATERIALS
    ANANI, A
    HUGGINS, RA
    [J]. JOURNAL OF POWER SOURCES, 1992, 38 (03) : 351 - 362
  • [2] ALL-SOLID LITHIUM ELECTRODES WITH MIXED-CONDUCTOR MATRIX
    BOUKAMP, BA
    LESH, GC
    HUGGINS, RA
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1981, 128 (04) : 725 - 729
  • [3] Amorphous silicon as a possible anode material for Li-ion batteries
    Bourderau, S
    Brousse, T
    Schleich, DM
    [J]. JOURNAL OF POWER SOURCES, 1999, 81 : 233 - 236
  • [4] Patterned metallization of porous silicon from electroless solution for direct electrical contact
    Gole, JL
    Seals, LT
    Lillehei, PT
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2000, 147 (10) : 3785 - 3789
  • [5] Structured silicon anodes for lithium battery applications
    Green, M
    Fielder, E
    Scrosati, B
    Wachtler, M
    Serra Moreno, J
    [J]. ELECTROCHEMICAL AND SOLID STATE LETTERS, 2003, 6 (05) : A75 - A79
  • [6] Kim I, 2000, ELECTROCHEM SOLID ST, V3, P493
  • [7] Development of a carbon-based lithium microbattery
    Kinoshita, K
    Song, X
    Kim, J
    Inaba, M
    [J]. JOURNAL OF POWER SOURCES, 1999, 81 : 170 - 175
  • [8] A high capacity nano-Si composite anode material for lithium rechargeable batteries
    Li, H
    Huang, XJ
    Chen, LQ
    Wu, ZG
    Liang, Y
    [J]. ELECTROCHEMICAL AND SOLID STATE LETTERS, 1999, 2 (11) : 547 - 549
  • [9] The crystal structural evolution of nano-Si anode caused by lithium insertion and extraction at room temperature
    Li, H
    Huang, XJ
    Chen, LQ
    Zhou, GW
    Zhang, Z
    Yu, DP
    Mo, YJ
    Pei, N
    [J]. SOLID STATE IONICS, 2000, 135 (1-4) : 181 - 191
  • [10] Si-O network encapsulated graphite-silicon mixtures as negative electrodes for lithium-ion batteries
    Ng, SB
    Lee, JY
    Liu, ZL
    [J]. JOURNAL OF POWER SOURCES, 2001, 94 (01) : 63 - 67