A mechanistic study of the hydrolytic stability of poly(2-(dimethylamino)ethyl methacrylate)

被引:292
作者
van de Wetering, P
Zuidam, NJ
van Steenbergen, MJ
van der Houwen, OAGJ
Underberg, WJM
Hennink, WE
机构
[1] Univ Utrecht, Fac Pharm, Utrecht Inst Pharmaceut Sci, Dept Pharmaceut, NL-3508 TB Utrecht, Netherlands
[2] Univ Utrecht, Fac Pharm, Res Sch Groningen Utrecht Inst Drug Explorat, NL-3508 TB Utrecht, Netherlands
关键词
D O I
10.1021/ma980689g
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The hydrolytic stability of poly(2-(dimethylamino)ethyl methacrylate) was investigated and compared with the stability of its monomer 2-(dimethylamino)ethyl methacrylate (DMAEMA), with 2-(dimethylamino)ethyl isobutyrate (DMAEIB), representing the repeating unit in the polymer, and with the related 3-(dimethylamino)propyl methacrylate (DMAPMA) (H-0/pH range -0.5 to +12, at 37 degrees C, in aqueous solution). At pH < 3, the unsaturated DMAEMA and DMAPMA were more stable than the saturated DMAEIB. At pH 4-8, DMAEMA and DMAEIB were equally stable, but less stable than DMAPMA. This has been ascribed to a coordination of the protonated dimethylamino group and the ester carbonyl, rendering the ester more susceptible to nucleophilic attack, of a hydroxyl ion. At alkaline pH (> pK(a)) no differences in stability between the compounds were found. P(DMAEMA), either in its free form or complexed to DNA, was substantially more stable to hydrolytic degradation than DMAEMA and DMAEIB. Fluorescence measurements performed with a copolymer of DMAEMA and dansyl ethyl methacrylamide showed that the dielectric constant (epsilon(r)) experienced in the environment of the polymer backbone, was low (about 7). This microenvironment might be the reason for the hydrolytic stability of the polymer, since the hydrolysis of the monomer decreased substantially with decreasing epsilon(r) of the medium. Accelerated degradation (80 degrees C, pH 1 and 7) of p(DMAEMA) and poly(2-(dimethylamino)ethyl acrylate), p(DMAEA), showed that p(DMAEA) was more sensitive to hydrolysis. This can be explained by the assumption that, due to the lack of the methyl group, the epsilon(r) in the environment of the acrylate backbone is higher than the epsilon(r) in the environment of the p(DMAEMA) backbone.
引用
收藏
页码:8063 / 8068
页数:6
相关论文
共 24 条
[21]   A GENERAL-APPROACH TO THE INTERPRETATION OF PH DEGRADATION PROFILES [J].
VANDERHOUWEN, OAGJ ;
BEIJNEN, JH ;
BULT, A ;
UNDERBERG, WJM .
INTERNATIONAL JOURNAL OF PHARMACEUTICS, 1988, 45 (03) :181-188
[22]   Degradation and release behavior of dextran-based hydrogels [J].
vanDijkWolthuis, WNE ;
Hoogeboom, JAM ;
vanSteenbergen, MJ ;
Tsang, SKY ;
Hennink, WE .
MACROMOLECULES, 1997, 30 (16) :4639-4645
[23]   Degradation kinetics cf methacrylated dextrans in aqueous solution [J].
vanDijkWolthuis, WNE ;
vanSteenbergen, MJ ;
Underberg, WJM ;
Hennink, WE .
JOURNAL OF PHARMACEUTICAL SCIENCES, 1997, 86 (04) :413-417
[24]  
WEAST RC, 1982, HDB CHEM PHYSICS, pD145