Amorphous silicoboron carbonitride ceramic with very high viscosity at temperatures above 1500°C

被引:229
作者
Riedel, R
Ruswisch, LM
An, LN
Raj, R
机构
[1] Tech Univ Darmstadt, Fachbereich Mat Wissensch, Fachgebiet Disperse Feststoffe, D-64287 Darmstadt, Germany
[2] Univ Colorado, Dept Mech Engn, Boulder, CO 80309 USA
关键词
D O I
10.1111/j.1151-2916.1998.tb02780.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Recently, the viscosity of a predominantly amorphous silicon carbonitride (Si1.7C1.0+/-0.1N1.5) alloy with an apparent glass-transition temperature (T-g) of 1400 degrees-1500 degrees C was studied. In this study, the creep behavior of silicoboron carbonitride (Si(2)B(1.0)C(3.4)N2(.3)), which seems to have a T(g)value of >1700 degrees C, was examined. Both materials exhibited a three-stage creep behavior. In stage I, the creep rate declined, because of densification, In stage II, the strain rate approaches a steady state. In stage III, it resumes a declining strain rate, which ultimately decreased below the measurement limit of the system. At 1550 degrees C in stage II, the viscosity of silicoboron carbonitride was six orders of magnitude higher than that of fused silica, Among the Si-C-N ceramics, only chemical-vapor-deposited and reaction-bonded silicon carbides seem to have greater creep resistance than the silicoboron carbonitrides at temperatures >1550 degrees C.
引用
收藏
页码:3341 / 3344
页数:4
相关论文
共 15 条
[1]  
An LA, 1998, J AM CERAM SOC, V81, P1349
[2]  
Baldus H, 1997, ANGEW CHEM, V109, P338
[3]   KINETICS AND MECHANISMS OF HIGH-TEMPERATURE CREEP IN SILICON-CARBIDE .1. REACTION-BONDED [J].
CARTER, CH ;
DAVIS, RF ;
BENTLEY, J .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1984, 67 (06) :409-417
[4]   KINETICS AND MECHANISMS OF HIGH-TEMPERATURE CREEP IN SILICON-CARBIDE .2. CHEMICALLY VAPOR-DEPOSITED [J].
CARTER, CH ;
DAVIS, RF ;
BENTLEY, J .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1984, 67 (11) :732-740
[5]  
DOREMUS RH, 1973, GLASS SCI, P106
[6]   SHEAR AND DENSIFICATION OF GLASS POWDER COMPACTS [J].
DUCAMP, VC ;
RAJ, R .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1989, 72 (05) :798-804
[7]   COMPRESSIVE CREEP OF SI3N4-MGO ALLOYS .1. EFFECT OF COMPOSITION [J].
LANGE, FF ;
DAVIS, BI ;
CLARKE, DR .
JOURNAL OF MATERIALS SCIENCE, 1980, 15 (03) :601-610
[8]   CAVITATION CONTRIBUTES SUBSTANTIALLY TO TENSILE CREEP IN SILICON-NITRIDE [J].
LUECKE, WE ;
WIEDERHORN, SM ;
HOCKEY, BJ ;
KRAUSE, RF ;
LONG, GG .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1995, 78 (08) :2085-2096
[9]   THE ELASTIC CONSTANTS OF A SOLID CONTAINING SPHERICAL HOLES [J].
MACKENZIE, JK .
PROCEEDINGS OF THE PHYSICAL SOCIETY OF LONDON SECTION B, 1950, 63 (361) :2-11
[10]  
RAJ R, 1981, J AM CERAM SOC, V64, pC143, DOI 10.1111/j.1151-2916.1981.tb10239.x