Synchrotron X-ray reflectivity study on the structure of templated polyorganosilicate thin films and their derived nanoporous analogues

被引:84
作者
Bolze, J
Ree, M
Youn, HS
Chu, SH
Char, K
机构
[1] Pohang Univ Sci & Technol, Ctr Integrated Mol Syst, Dept Chem, Pohang 790784, South Korea
[2] Pohang Univ Sci & Technol, Ctr Integrated Mol Syst, Pohang 790784, South Korea
[3] BK21 Funct Polymer Thin Film Grp, Pohang 790784, South Korea
[4] Pohang Accelerator Lab, Pohang 790784, South Korea
[5] Seoul Natl Univ, Sch Chem Engn, Kwanak Gu, Seoul 151742, South Korea
关键词
Carrier concentration - Electromagnetic wave reflection - Permittivity - Silicates - Silicon wafers - Spin coating - Surface roughness - Synchrotron radiation - Thermal effects - Thin films - X rays;
D O I
10.1021/la010451c
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Comprehensive X-ray reflectivity (XR) studies were conducted to characterize the structure of thin polyalkylsilicate films made of a poly(methylsilsesquioxane-co-ethylenylsilsesquioxane) precursor containing a star-shaped poly(epsilon -caprolactone) as a pore generator (porogen). The films were deposited on silicon wafer substrates by spin-coating and subsequently cured at various temperatures. Such spin-on glasses have a potential application as a low-dielectric-constant material for advanced semiconductors. Because high-intensity synchrotron X-ray radiation was used, the XR data could be measured over 9 orders of magnitude in intensity, which facilitated the observation of fine structural details. A hierarchical fitting procedure for modeling the XR data is given. By evaluation of the critical angle of total reflection of the film material, which was observed at smallest angles, in particular the film electron density could be determined with a high accuracy. The films cured at 420 degreesC show a lower electron density as compared to those cured at 250 degreesC. This is explained by the fact that at the higher temperature the porogen is calcined and escapes from the films leaving behind a nanoporous structure. Film porosities could be estimated from the observed changes in the electron densities. From the very large number of high-frequency oscillations observed in the XR curves, it is concluded that the films exhibit a homogeneous, well-defined structure with small interface and surface roughness. The film thickness could be determined with an accuracy of +/-1 Angstrom. The observation of an additional low-frequency modulation of the XR curves revealed a surface skin layer with a thickness of ca. 45 Angstrom and with a slightly increased" electron density as compared to the bulk of the film.
引用
收藏
页码:6683 / 6691
页数:9
相关论文
共 34 条
[31]   Study of ultra-thin hydrogen silsesquioxane films using x-ray reflectivity [J].
Wu, WL ;
Liou, HC .
THIN SOLID FILMS, 1998, 312 (1-2) :73-77
[32]  
Ying JY, 1999, ANGEW CHEM INT EDIT, V38, P56, DOI 10.1002/(SICI)1521-3773(19990115)38:1/2<56::AID-ANIE56>3.0.CO
[33]  
2-E
[34]   X-RAY-REFLECTIVITY STUDY OF THE COPPER-WATER INTERFACE IN A TRANSMISSION GEOMETRY UNDER INSITU ELECTROCHEMICAL CONTROL [J].
YOU, H ;
MELENDRES, CA ;
NAGY, Z ;
MARONI, VA ;
YUN, W ;
YONCO, RM .
PHYSICAL REVIEW B, 1992, 45 (19) :11288-11298