Grain boundary blocking effect in tetragonal yttria stabilized zirconia

被引:40
作者
Santos, AP
Domingues, RZ
Kleitz, M
机构
[1] INPG, Lab Electrochim & Physicochim Mat & Interfaces, F-38402 St Martin Dheres, France
[2] CNRS, F-38402 St Martin Dheres, France
[3] Univ Fed Minas Gerais, Dept Quim, BR-31270901 Belo Horizonte, MG, Brazil
关键词
TZP; grain growth; grain boundaries; blocking effect; impedance spectroscopy;
D O I
10.1016/S0955-2219(98)00017-X
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
samples of yttria stabilized tetragonal zirconia, with different grain sizes have been synthesized. Care was taker? to avoid the presence of any trace of monoclinic zirconia. The features of their grain boundary blocking effect are compared to those of YSZ samples of similar purity. Certain variation laws of the blocking effects are quasi identical, especially some dependences on the grain size. The most significant differences concern the variation of the blocking factor with temperature and the transition to the so-called intrinsic regime. In tetragonal zirconia, the blocking factor continuously decreases in the temperature interval 150-600 degrees C and the onset of the intrinsic regime could occur at a smaller grain size of about 0.9 mu m. (C) 1998 Elsevier Science Limited All rights reserved.
引用
收藏
页码:1571 / 1578
页数:8
相关论文
共 34 条
[21]   ELECTRICAL-CONDUCTIVITY OF YTTRIA-STABILIZED ZIRCONIA SINGLE-CRYSTALS [J].
IKEDA, S ;
SAKURAI, O ;
UEMATSU, K ;
MIZUTANI, N ;
KATO, M .
JOURNAL OF MATERIALS SCIENCE, 1985, 20 (12) :4593-4600
[22]   TETRAGONAL ZIRCONIA - WET CHEMICAL PREPARATION, MECHANICAL AND ELECTRICAL-PROPERTIES [J].
KEIZER, K ;
VANHEMERT, M ;
VANDEGRAAF, MACG ;
BURGGRAAF, AJ .
SOLID STATE IONICS, 1985, 16 (1-4) :67-72
[23]   MODEL FOR ION-BLOCKING AT INTERNAL INTERFACES IN ZIRCONIAS [J].
KLEITZ, M ;
DESSEMOND, L ;
STEIL, MC .
SOLID STATE IONICS, 1995, 75 :107-115
[24]  
KLEITZ M, 1993, SCI TECHNOLOGY ZIRCO, V5, P593
[25]   DEGRADATION OF THE ELECTRICAL-PROPERTIES OF Y2O3 PARTIALLY-STABILIZED ZIRCONIA CERAMICS OWING TO MICROCRACKING DURING ANNEALING [J].
KUWABARA, M ;
ASHIZUKA, M ;
KUBOTA, Y ;
TSUKIDATE, T .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1986, 5 (01) :7-9
[26]   Impedance spectroscopy of Mg-partially stabilized zirconia and cubic phase decomposition [J].
Muccillo, ENS ;
Kleitz, M .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1996, 16 (04) :453-465
[27]  
NAVARRO LM, 1983, 4 EUROCERAMICS, V5, P395
[28]   Production of defect-poor nanostructured ceramics of yttria-zirconia [J].
SagelRansijn, CD ;
Winnubst, AJA ;
Kerkwijk, B ;
Burggraaf, AJ ;
Verweij, H .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1997, 17 (06) :831-841
[29]   Crystallite growth in yttria-doped superfine zirconia powders and their compacts: A comparison between Y-TZP and YSZ [J].
Shi, JL ;
Ruan, ML ;
Yen, TS .
CERAMICS INTERNATIONAL, 1996, 22 (02) :137-142
[30]   Densification of yttria-stabilized zirconia - Impedance spectroscopy analysis [J].
Steil, MC ;
Thevenot, F ;
Kleitz, M .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (01) :390-398