Advances in ceramic composites reinforced by continuous fibers

被引:41
作者
Cox, BN [1 ]
Zok, FW [1 ]
机构
[1] UNIV CALIF SANTA BARBARA, DEPT MAT, SANTA BARBARA, CA 93106 USA
关键词
D O I
10.1016/S1359-0286(96)80049-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ceramic matrix composites reinforced with continuous fibers are on the verge of insertion into hot engineering structures. Yet current research is only beginning to attack some of the most critical problems. Key developments in the last 24 months include the formulation of constitutive laws for continuum mechanics analyses; the discovery of stable weak oxide-oxide interface systems; the analysis of how fiber creep limits life at high temperatures; confrontation of the problem of oxidation pesting at intermediate temperatures in SiC based systems; re-examination of the maxim that interfaces must be weak; and the advent of textile reinforcement as the solution to delamination problems. (C) Current Chemistry Ltd
引用
收藏
页码:666 / 673
页数:8
相关论文
共 92 条
[81]   DIRECT OBSERVATION OF THE FRACTURE OF CAS-GLASS SIC COMPOSITES .1. DELAMINATION [J].
SHERCLIFF, HR ;
VEKINIS, G ;
BEAUMONT, PWR .
JOURNAL OF MATERIALS SCIENCE, 1994, 29 (14) :3643-3652
[82]   DIRECT OBSERVATION OF THE FRACTURE OF CAS-GLASS SIC COMPOSITES .2. NOTCHED TENSION [J].
SHERCLIFF, HR ;
BEAUMONT, PWR ;
VEKINIS, G .
JOURNAL OF MATERIALS SCIENCE, 1994, 29 (16) :4184-4190
[83]   SIC FIBRE/BOROSILICATE GLASS COMPOSITE .2. FACTORS CONTROLLING THE MECHANICAL-PROPERTIES [J].
SHIN, DW ;
AUH, KH ;
KNOWLES, KM .
JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1995, 103 (05) :409-417
[84]   Effect of loading rate on the monotonic tensile behavior of a continuous-fiber-reinforced glass-ceramic matrix composite [J].
Sorensen, BF ;
Holmes, JW .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (02) :313-320
[85]   Concept for a damage-tolerant ceramic composite with ''strong'' interfaces [J].
Tu, WC ;
Lange, FF ;
Evans, AG .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (02) :417-424
[86]   RELATIONSHIPS BETWEEN HYSTERESIS MEASUREMENTS AND THE CONSTITUENT PROPERTIES OF CERAMIC-MATRIX COMPOSITES .1. THEORY [J].
VAGAGGINI, E ;
DOMERGUE, JM ;
EVANS, AG .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1995, 78 (10) :2709-2720
[87]   Characterization of microstructure and tensile behavior of a cross-woven C-SiC composite [J].
Wang, M ;
Laird, C .
ACTA MATERIALIA, 1996, 44 (04) :1371-1387
[88]   Damage and fracture of a cross woven C/SiC composite subject to compression loading [J].
Wang, MD ;
Laird, C .
JOURNAL OF MATERIALS SCIENCE, 1996, 31 (08) :2065-2069
[89]   HIGH-TEMPERATURE DEFORMATION AND RUPTURE IN SIC-C COMPOSITES [J].
WEBER, CH ;
KIM, KT ;
HEREDIA, FE ;
EVANS, AG .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 196 (1-2) :25-31
[90]   CREEP ANISOTROPY OF A CONTINUOUS-FIBER-REINFORCED SILICON-CARBIDE CALCIUM ALUMINOSILICATE COMPOSITE [J].
WEBER, CH ;
LOFVANDER, JPA ;
EVANS, AG .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (07) :1745-1752