Strength and ductility of as-plated and sintered CVD nickel foams

被引:36
作者
Olurin, OB
Wilkinson, DS [1 ]
Weatherly, GC
Paserin, V
Shu, J
机构
[1] McMaster Univ, Dept Mat Sci & Engn, Hamilton, ON L8S 4L7, Canada
[2] ITSL, Mississauga, ON L5K 1Z9, Canada
关键词
open cell; foam; chemical vapor deposition; sintering; mechanical properties; microstructural characterization; batteries; hybrid electric vehicles;
D O I
10.1016/S0266-3538(03)00265-3
中图分类号
TB33 [复合材料];
学科分类号
摘要
Low density, open cell nickel foams produced by chemical vapor deposition (CVD) are made for electrochemical applications. One process involves nickel carbonyl decomposition within a plater whereby nickel is deposited onto a reticulated polyurethane (PU) foam substrate. The as-plated nickel foams are then sintered in a partially reducing atmosphere at high temperature in order to enhance ductility. The high strength and brittleness of the as-plated foams presents a material handling challenge in manufacturing. As-plated foams are much stronger than sintered foams of the same density. Our analysis shows that the strengthening in the as-plated nickel foams is due to a combination of grain size, solid solution strengthening, dislocations and nano-porosity. Of these, the effects due to interstitial carbon are dominant. This is lost upon sintering. Foam ductility does not show the usual inverse trend with strength. Instead, foam ductility and bendability show little variation with carbon or sulfur level or with the level of nano-porosity, which are among the strongest strengthening sources in the foams. (C) 2003 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2317 / 2329
页数:13
相关论文
共 43 条
[21]  
HILL R, 1989, MATH THEORY OFPLASTI
[22]  
Honeycombe R. W. K., 1985, PLASTIC DEFORMATION
[23]   HALL-PETCH STRENGTHENING FOR THE MICROHARDNESS OF 12 NANOMETER GRAIN DIAMETER ELECTRODEPOSITED NICKEL [J].
HUGHES, GD ;
SMITH, SD ;
PANDE, CS ;
JOHNSON, HR ;
ARMSTRONG, RW .
SCRIPTA METALLURGICA, 1986, 20 (01) :93-97
[24]   THE HALL-PETCH RELATIONSHIPS IN MECHANICALLY ALLOYED NI3AL WITH OXIDE DISPERSOIDS [J].
JANG, JSC ;
KOCH, CC .
SCRIPTA METALLURGICA, 1988, 22 (05) :677-682
[25]   CONFIRMATION OF SULFUR EMBRITTLEMENT IN NICKEL-ALLOYS [J].
JOHNSON, WC ;
DOHERTY, JE ;
KEAR, BH ;
GIAMEI, AF .
SCRIPTA METALLURGICA, 1974, 8 (08) :971-974
[26]  
Kelly A., 1971, Strengthening Methods in Crystals
[27]  
KOCKS UF, 1975, PROG MATER SCI, V19, P1
[28]  
KOCKS UF, 1980, STRENGTH METALS ALLO, P1661
[29]   THE INFLUENCE OF GRAIN-BOUNDARY SULFUR CONCENTRATION ON THE INTERGRANULAR BRITTLENESS OF NICKEL OF DIFFERENT PURITIES [J].
LOIER, C ;
BOOS, JY .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1981, 12 (07) :1223-1233
[30]   WORK HARDENING AND DISLOCATION ARRANGEMENT OF FCC SINGLE CRYSTALS .2. ELECTRON MICROSCOPE TRANSMISSION STUDIES OF NI-CO SINGLE CRYSTALS AND RELATION TO WORK-HARDENING THEORY [J].
MADER, S ;
THIERINGER, HM ;
SEEGER, A .
JOURNAL OF APPLIED PHYSICS, 1963, 34 (11) :3376-&