Effect of heat treatment on morphology, crystalline structure and photocatalysis properties of TiO2 nanotubes on Ti substrate and freestanding membrane

被引:155
作者
Fang, Dong [1 ,3 ]
Luo, Zhiping [2 ]
Huang, Kelong [1 ]
Lagoudas, Dimitris C. [3 ]
机构
[1] Cent S Univ, Coll Chem & Chem Engn, Changsha 410083, Hunan, Peoples R China
[2] Texas A&M Univ, Microscopy & Imaging Ctr, College Stn, TX 77843 USA
[3] Texas A&M Univ, Dept Aerosp Engn, College Stn, TX 77843 USA
基金
中国国家自然科学基金;
关键词
TiO2 nanotube arrays; Anodic oxidation; Calcination; Phase transformation; Photocatalysis; ANATASE-RUTILE TRANSFORMATION; PHOTOELECTROCHEMICAL PROPERTIES; CALCINATION TEMPERATURE; TITANIA NANOTUBES; MU-M; ARRAYS; ANODIZATION; DEGRADATION; FABRICATION; MECHANISM;
D O I
10.1016/j.apsusc.2011.02.037
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Highly ordered titanium oxide (TiO2) nanotubes were prepared by electrolytic anodization of titanium electrodes. Morphological evolution and phase transformations of TiO2 nanotubes on a Ti substrate and that of freestanding TiO2 membranes during the calcinations process were studied by scanning electron microscopy, transmission electron microscopy, and X-ray diffraction microscopy. The detailed results and mechanisms on the morphology and crystalline structure were presented. Our results show that a compact layer exists between the tubular layer and Ti substrate at 600 degrees C, and the length of the nanotubes shortens dramatically at 750 degrees C. The freestanding membranes have many particles on their tubes during calcinations from 450 to 900 degrees C. The TiO2 nanotubes on the Ti substrate transform to rutile crystals at 600 degrees C, while the freestanding TiO2 membranes retain an anatase crystal with increasing temperature to 800 degrees C. The photocatalytic activity of TiO2 nanotubes on a Ti substrate annealed at different temperatures was investigated by the degradation of methyl orange in aqueous solution under UV light irradiation. Due to the anatase crystals in the tubular layer and rutile crystals in the compact layer, TiO2 nanotubes annealed at 450 degrees C with pure anatase crystals have a better photocatalytic activity than those annealed at 600 degrees C or 750 degrees C. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:6451 / 6461
页数:11
相关论文
共 52 条
[1]   Self-organized, free-standing TiO2 nanotube membrane for flow-through photocatalytic applications [J].
Albu, Sergiu P. ;
Ghicov, Andrei ;
Macak, Jan M. ;
Hahn, Robert ;
Schmuki, Patrik .
NANO LETTERS, 2007, 7 (05) :1286-1289
[2]   Room Temperature One-Step Polyol Synthesis of Anatase TiO2 Nanotube Arrays: Photoelectrochemical Properties [J].
Allam, Nageh K. ;
Grimes, Craig A. .
LANGMUIR, 2009, 25 (13) :7234-7240
[3]   Anatase-to-rutile transition of titania thin films prepared by MOCVD [J].
Byun, C ;
Jang, JW ;
Kim, IT ;
Hong, KS ;
Lee, BW .
MATERIALS RESEARCH BULLETIN, 1997, 32 (04) :431-440
[4]   Titanium dioxide nanomaterials: Synthesis, properties, modifications, and applications [J].
Chen, Xiaobo ;
Mao, Samuel S. .
CHEMICAL REVIEWS, 2007, 107 (07) :2891-2959
[5]  
Choi YS, 2000, J CHEM TECHNOL BIOT, V75, P1145, DOI 10.1002/1097-4660(200012)75:12<1145::AID-JCTB341>3.0.CO
[6]  
2-X
[7]   MECHANISM OF THE INHIBITING EFFECT OF PHOSPHATE ON THE ANATASE-]RUTILE TRANSFORMATION INDUCED BY THERMAL AND MECHANICAL TREATMENT OF TIO2 [J].
CRIADO, J ;
REAL, C .
JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS I, 1983, 79 :2765-2771
[8]   Study on the Anatase to Rutile Phase Transformation and Controlled Synthesis of Rutile Nanocrystals with the Assistance of Ionic Liquid [J].
Ding, Kunlun ;
Miao, Zhenjiang ;
Hu, Baoji ;
An, Guimin ;
Sun, Zhenyu ;
Han, Buxing ;
Liu, Zhimin .
LANGMUIR, 2010, 26 (12) :10294-10302
[9]   Grain growth enhanced by anatase-to-rutile transformation in gel-derived nanocrystalline titania powders [J].
Ding, Xing-zhao ;
Liu, Xiang-huai .
Journal of Alloys and Compounds, 1997, 248 (1-2) :143-145
[10]   Electrochemical properties of ordered TiO2 nanotube loaded with Ag nano-particles for lithium anode material [J].
Fang, Dong ;
Huang, Kelong ;
Liu, Shuqin ;
Li, Zhaojian .
JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 464 (1-2) :L5-L9