Comparative evaluation of thione and phosphate monomers on bonding gold alloy and Ti-6Al-7Nb alloy with tri-n-butylborane initiated resin

被引:17
作者
Ishii, Takaya [2 ]
Koizumi, Hiroyasu [1 ,3 ]
Yoneyama, Takayuki [4 ]
Tanoue, Naomi [5 ]
Ishikawa, Yumi [1 ]
Matsumura, Hideo [1 ,3 ]
机构
[1] Nihon Univ, Sch Dent, Dept Fixed Prosthodont, Chiyoda Ku, Tokyo 1018310, Japan
[2] Nihon Univ, Grad Sch Dent, Chiyoda Ku, Tokyo 1018310, Japan
[3] Nihon Univ, Sch Dent, Div Adv Dent Treatment,Dent Res Ctr, Chiyoda Ku, Tokyo 1018310, Japan
[4] Tokyo Med & Dent Univ, Dept Met, Inst Biomat & Bioengn, Chiyoda Ku, Tokyo 1010062, Japan
[5] Nagasaki Univ, Hosp Med & Dent, Dept Specialized Dent, Nagasaki 8528501, Japan
关键词
phosphate; thione; Ti-6Al-7Nb alloy;
D O I
10.4012/dmj.27.56
中图分类号
R78 [口腔科学];
学科分类号
1003 [口腔医学];
摘要
This study aimed to evaluate the bonding behaviors of a gold alloy and a titanium-aluminum-niobium (Ti-6Al-7Nb) alloy after priming with three metal conditioners. Cast alloy disks were ground and divided into the following four conditions: (1) unprimed control versus priming with (2) Alloy Primer, (3) Estenia Opaque Primer, or (4) V-Primer. The disks were bonded with tri-n-butylborane (TBB) initiated methacrylic resin, and shear bond strengths were determined both before and after 20,000 times of thermocycling. Alloy Primer and V-Primer - which contained a vinyl-thione monomer - were effective for bonding the Au-Pt-Pd alloy. As for the hydrophobic phosphate monomer contained in Alloy Primer and Estenia Opaque Primer, it was effective for bonding the Ti-6Al-7Nb alloy. Further, when specimens were primed with Alloy Primer that contained both functional monomers, bond strength to Ti-6Al-7Nb alloy was greater than that to Au-Pt-Pd alloy.
引用
收藏
页码:56 / 60
页数:5
相关论文
共 25 条
[1]
BONDING FIXED PROSTHODONTIC COMPOSITE RESIN AND PRECIOUS METAL-ALLOYS WITH THE USE OF A VINYL-THIOL PRIMER AND AN ADHESIVE OPAQUE RESIN [J].
ATSUTA, M ;
MATSUMURA, H ;
TANAKA, T .
JOURNAL OF PROSTHETIC DENTISTRY, 1992, 67 (03) :296-300
[2]
Acid etching of titanium for bonding with veneering composite resins [J].
Ban, Seiji ;
Taniki, Toshio ;
Sato, Hideo ;
Kono, Hiroshi ;
Iwaya, Yukari ;
Miyamoto, Motoharu .
DENTAL MATERIALS JOURNAL, 2006, 25 (02) :382-390
[3]
HANSSON O, 1993, SCAND J DENT RES, V101, P243
[4]
International Organization for Standardization, 1994, ISO TR 11405
[5]
Bond strength to primed Ti-6Al-7Nb alloy of two acrylic resin adhesives [J].
Koizumi, Hiroyasu ;
Furuchi, Mika ;
Tanoue, Naomi ;
Yanagida, Hiroaki ;
Yoneyama, Takayuki ;
Matsumura, Hideo .
DENTAL MATERIALS JOURNAL, 2006, 25 (02) :286-290
[6]
Bonding of a cobalt-chromium alloy with acidic primers and tri-n-butylborane-initiated luting agents [J].
Matsumura, H ;
Tanaka, T ;
Taira, Y ;
Atsuta, M .
JOURNAL OF PROSTHETIC DENTISTRY, 1996, 76 (02) :194-199
[7]
EFFECT OF AN ADHESIVE PRIMER ON THE INTEGRITY OF OCCLUSAL VENEER-METAL INTERFACE AND WEAR OF COMPOSITE RESIN VENEERED RESTORATIONS [J].
MATSUMURA, H ;
LEINFELDER, KF .
JOURNAL OF PROSTHETIC DENTISTRY, 1993, 70 (04) :296-299
[8]
ADHESIVE BONDING OF TITANIUM WITH A TITANATE COUPLER AND 4-META MMA-TBB OPAQUE RESIN [J].
MATSUMURA, H ;
YOSHIDA, K ;
TANAKA, T ;
ATSUTA, M .
JOURNAL OF DENTAL RESEARCH, 1990, 69 (09) :1614-1616
[9]
Effect of acidic primers on bonding between stainless steel and auto-polymerizing methacrylic resins [J].
Matsumura, H ;
Tanaka, T ;
Atsuta, M .
JOURNAL OF DENTISTRY, 1997, 25 (3-4) :285-290
[10]
Veneering technique for a Ti-6A1-7Nb framework used in a resin-bonded fixed partial denture with a highly filled indirect composite [J].
Matsumura, H ;
Yoneyama, T ;
Shimoe, S .
JOURNAL OF PROSTHETIC DENTISTRY, 2002, 88 (06) :636-639