Effect of metal compounds on thermal degradation behavior of aliphatic poly(hydroxyalkanoic acid)s

被引:49
作者
Kim, Kang Ju [2 ]
Doi, Yoshihm [1 ]
Abe, Hideki [1 ,2 ]
机构
[1] Riken Inst Phys & Chem Res, Chem Anal Team, Wako, Saitama 3510198, Japan
[2] Tokyo Inst Technol, Dept Innovat & Engineered Mat, Midori Ku, Yokohama, Kanagawa 2268502, Japan
关键词
thermal degradation; aliphatic polyester; poly(hydroxyalkanoic acid); metal compound; random chain scission; cyclic rupture;
D O I
10.1016/j.polymdegradstab.2008.01.026
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Effect of metal compounds on the thermal degradation behaviors of poly(3-hydroxybutyric acid) (P(3HB)), poly(4-hydroxybutyric acid) (P(4HB)), and poly(epsilon-caprolactone) (PCL) was investigated by means of thermogravimetric and pyrolysis-gas chromatograph mass spectrometric analyses. Na and Ca compounds accelerated a random chain scission of P(3HB) molecules resulting in a decrease of thermal degradation temperature, whereas the contribution of Zn, Sn, Al compounds to the thermal degradation of P(3HB) was very small. In contrast to P(3HB), Zn, Sn and Al compounds induced the thermal degradation of PCL at lower temperature range by catalyzing the selective unzipping depolymerization from omega-hydroxyl chain end. Transesterification reaction of PCL molecules could be facilitated by the presence of Ca compound, while the gravimetric change was detected at almost identical temperature region regardless of the content of Ca compound. According to the lactonizing characteristic of monomer unit, the thermal degradation of P(4HB) progressed by the cyclic rupture via unzipping reaction from the w-hydroxyl chain end or/and random intramolecular transesterification at the main chain with a release of gamma-butyrolactone as volatile product. Each of metal compounds used in this study was effective to catalyze the cyclic rupture of P(4HB) molecules, and the degradation rate was accelerated by the presence of metal compounds. (c) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:776 / 785
页数:10
相关论文
共 46 条
[1]   SEPARATION AND STRUCTURAL CHARACTERIZATION OF CYCLIC AND OPEN-CHAIN OLIGOMERS PRODUCED IN THE PARTIAL PYROLYSIS OF MICROBIAL POLY(HYDROXYBUTYRATES) [J].
ABATE, R ;
BALLISTRERI, A ;
MONTAUDO, G ;
GIUFFRIDA, M ;
IMPALLOMENI, G .
MACROMOLECULES, 1995, 28 (23) :7911-7916
[2]   Thermal degradation processes of end-capped poly(L-lactide)s in the presence and absence of residual zinc catalyst [J].
Abe, H ;
Takahashi, N ;
Kim, KJ ;
Mochizuki, M ;
Doi, Y .
BIOMACROMOLECULES, 2004, 5 (04) :1606-1614
[3]   Effects of residual zinc compounds and chain-end structure on thermal degradation of poly(ε-caprolactone) [J].
Abe, H ;
Takahashi, N ;
Kim, KJ ;
Mochizuki, M ;
Doi, Y .
BIOMACROMOLECULES, 2004, 5 (04) :1480-1488
[4]   Thermal degradation of environmentally degradable poly(hydroxyalkanoic acid)s [J].
Abe, Hideki .
MACROMOLECULAR BIOSCIENCE, 2006, 6 (07) :469-486
[5]   Recent developments in ring opening polymerization of lactones for biomedical applications [J].
Albertsson, AC ;
Varma, IK .
BIOMACROMOLECULES, 2003, 4 (06) :1466-1486
[6]   Thermal degradation of poly[(R)-3-hydroxybutyrate], poly[ε-caprolactone], and poly[(S)-lactide] [J].
Aoyagi, Y ;
Yamashita, K ;
Doi, Y .
POLYMER DEGRADATION AND STABILITY, 2002, 76 (01) :53-59
[7]   Influence of residual monomers and metals on poly (L-lactide) thermal stability [J].
Cam, D ;
Marucci, M .
POLYMER, 1997, 38 (08) :1879-1884
[8]  
DUDA A, 2002, BIOPOLYMERS B, V3, P371
[9]   Thermal stability of poly (L-lactide): influence of end protection by acetyl group [J].
Fan, YJ ;
Nishida, H ;
Shirai, Y ;
Endo, T .
POLYMER DEGRADATION AND STABILITY, 2004, 84 (01) :143-149
[10]   Thermal degradation of poly(L-lactide): effect of alkali earth metal oxides for selective L,L-lactide formation [J].
Fan, YJ ;
Nishida, H ;
Mori, T ;
Shirai, Y ;
Endo, T .
POLYMER, 2004, 45 (04) :1197-1205