Membrane and active layer degradation following PEMFC steady-state operation -: II.: Influence of Ptz+ on membrane properties

被引:44
作者
Iojoiu, C. [1 ]
Guilminot, E.
Maillard, F.
Chatenet, M.
Sanchez, J. -Y.
Claude, E.
Rossinot, E.
机构
[1] UJF, Lab Electrochim & Physicochim Mat & Interfaces, UMR 5631, CNRS,INPG, F-38402 St Martin Dheres, France
[2] Axane Air Liquide, F-38360 Sassenage, France
关键词
D O I
10.1149/1.2775282
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
This paper (Part II) aims to provide an understanding of the degradations originating in the membrane or the binder and which dramatically affect the membrane electrode assembly performance and therefore the lifespan of protein exchange memory fuel cells. In Part I, evidence was provided of the corrosion of the platinum catalysts and the diffusion/migration through the membrane of platinum cations. In this paper we establish that these platinum cations induce physical cross-links that modify both the thermomechanical properties and the conductivities of the membrane. Since physical cross-links are reversible, ex situ experiments were performed to recover the performance of pristine membranes by acidic treatment. Membrane performance was found to be much more affected in the case of membranes aged in the hot zone rather than in the cold zone.
引用
收藏
页码:B1115 / B1120
页数:6
相关论文
共 28 条
[1]   Synthesis, characterization, and crystal structures of the osmium triflate complexes Cp*Os(P-P)(OTf) and [Cp*Os(P-P)(OH2)][OTf] [J].
Brumaghim, Julia L. ;
Gross, Christopher L. ;
Girolami, Gregory S. .
JOURNAL OF ORGANOMETALLIC CHEMISTRY, 2006, 691 (18) :3874-3880
[2]   Operating proton exchange membrane fuel cells without external humidification of the reactant gases - Fundamental aspects [J].
Buchi, FN ;
Srinivasan, S .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (08) :2767-2772
[3]   Advanced materials for improved PEMFC performance and life [J].
Curtin, DE ;
Lousenberg, RD ;
Henry, TJ ;
Tangeman, PC ;
Tisack, ME .
JOURNAL OF POWER SOURCES, 2004, 131 (1-2) :41-48
[4]   Kinetic model of platinum dissolution in PEMFCs [J].
Darling, RM ;
Meyers, JP .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2003, 150 (11) :A1523-A1527
[5]   Degradation study of MEA for PEMFCs under low humidity conditions [J].
Endoh, E ;
Terazono, S ;
Widjaja, H ;
Takimoto, Y .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2004, 7 (07) :A209-A211
[6]   Structural evolution of water swollen perfluorosulfonated ionomers from dry membrane to solution [J].
Gebel, G .
POLYMER, 2000, 41 (15) :5829-5838
[7]   SWELLING STUDY OF PERFLUOROSULPHONATED IONOMER MEMBRANES [J].
GEBEL, G ;
ALDEBERT, P ;
PINERI, M .
POLYMER, 1993, 34 (02) :333-339
[8]   Detection of Ptz+ ions and Pt nanoparticles inside the membrane of a used PEMFC [J].
Guilminot, E. ;
Corcella, A. ;
Charlot, F. ;
Maillard, F. ;
Chatenet, M. .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2007, 154 (01) :B96-B105
[9]   Aspects of the chemical degradation of PFSA ionomers used in PEM fuel cells [J].
Healy, J ;
Hayden, C ;
Xie, T ;
Olson, K ;
Waldo, R ;
Brundage, A ;
Gasteiger, H ;
Abbott, J .
FUEL CELLS, 2005, 5 (02) :302-308
[10]   Mechanical endurance of polymer electrolyte membrane and PEM fuel cell durability [J].
Huang, Xinyu ;
Solasi, Roham ;
Zou, Yue ;
Feshler, Matthew ;
Reifsnider, Kenneth ;
Condit, David ;
Burlatsky, Sergei ;
Madden, Thomas .
JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 2006, 44 (16) :2346-2357