Crack-healing behavior under stress of mullite/silicon carbide ceramics and the resultant fatigue strength

被引:78
作者
Ando, K [1 ]
Furusawa, K [1 ]
Chu, MC [1 ]
Hanagata, T [1 ]
Tuji, K [1 ]
Sato, S [1 ]
机构
[1] Yokohama Natl Univ, Dept Energy & Safety Engn, Yokohama, Kanagawa 240, Japan
关键词
D O I
10.1111/j.1151-2916.2001.tb00960.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Mullite/SiC composite ceramics were sintered and subjected to three-point bending of specimens made according to the appropriate JIS standard. A semicircular surface crack 100 to 250 Rm in diameter was made on each specimen. We systematically studied crack-healing behavior and cyclic- and static-fatigue strengths at room temperature and 1000 degreesC (crack-healing temperature) by using three types of specimens (smooth, cracked, and crack-healed). The main conclusions are as follows: (i) mullite/SiC composite ceramics have the ability to heal after cracking; (ii) crack-healed specimens exhibited higher static and fatigue strengths than those of smooth specimens, which was caused by crack-healing; (iii) a sample crack-healed at 1000 degreesC had a high fatigue strength at 1000 degreesC; and (iv) mullite/SiC ceramics can heal a crack under stress at 1000 degreesC, and this behavior was considered using crack-driving force and crack-healing force, qualitatively.
引用
收藏
页码:2073 / 2078
页数:6
相关论文
共 23 条
[1]   Fatigue strength of crack-healed Si3N4/SiC composite ceramics [J].
Ando, K ;
Chu, MC ;
Yao, F ;
Sato, S .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1999, 22 (10) :897-903
[2]   A preliminary study on crack healing behaviour of Si3N4/SiC composite ceramics [J].
Ando, K ;
Ikeda, T ;
Sato, S ;
Yao, F ;
Kobayasi, Y .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1998, 21 (01) :119-122
[3]  
Ando K, 2000, STRUCTURAL INTEGRITY IN THE 21ST CENTURY, P345
[4]   Effect of pre-crack size and testing temperature on fatigue strength properties of crack healed mullite [J].
Ando, K. ;
Tuji, K. ;
Furusawa, K. ;
Hanagata, T. ;
Chu, M.-C. ;
Sato, S. .
Zairyo/Journal of the Society of Materials Science, Japan, 2001, 50 (08) :920-925
[5]  
Ando K, 1998, ECF 12: FRACTURE FROM DEFECTS, VOLS. I-III, P497
[6]  
Ando K., 1999, Journal of the Society of Materials Science, Japan, V48, P1173, DOI 10.2472/jsms.48.1173
[7]  
Ando K., 1999, JPN SOC MECH ENG, V65, P1132
[8]  
Ando K., 1998, JPN SOC MECH ENG, V64, P1936
[9]   CRACK HEALING BEHAVIOR OF HOT-PRESSED SILICON-NITRIDE DUE TO OXIDATION [J].
CHOI, SR ;
TIKARE, V .
SCRIPTA METALLURGICA ET MATERIALIA, 1992, 26 (08) :1263-1268
[10]  
CHU MC, 1995, FATIGUE FRACT ENG M, V18, P1019, DOI 10.1111/j.1460-2695.1995.tb00924.x