Versatility of biodegradable biopolymers: degradability and an in vivo application

被引:94
作者
Hasirci, V [1 ]
Lewandrowski, K
Gresser, JD
Wise, DL
Trantolo, DJ
机构
[1] Middle E Tech Univ, Dept Biol Sci, Biotechnol Res Unit, TR-06531 Ankara, Turkey
[2] Massachusetts Gen Hosp, Orthopaed Res Labs, Boston, MA 02114 USA
[3] Cambridge Sci Inc, Belmont, MA 02478 USA
关键词
biodegradation; interpenetrating networks; molecular reinforcement; osteointegration; polypropylene fumarate;
D O I
10.1016/S0168-1656(00)00409-0
中图分类号
Q81 [生物工程学(生物技术)]; Q93 [微生物学];
学科分类号
071005 ; 0836 ; 090102 ; 100705 ;
摘要
Biodegradable materials have various important applications in the biomedical field. There are basically two groups of polyesters which have significant importance in this field. These are polylactides and polyhydroxybutyrates. Both groups degrade via hydrolysis with the rates of degradation depending on medium properties such as pH, temperature, solvent and presence of biocatalysts, as well as on chemical compositions. In order for these biomaterials to be suitable for use in load bearing applications without deformation or warping their strengths and their capability to maintain their form must be improved. To insure dimensional stability during degradation and to match modulus and strength to that of bone, introduction of a reinforcing structure for those applications to plate fixation through the creation of an interpenetrating network might be a feasible approach. In this study, poly(lactide-co-glycolide) (PLGA), was the major structural element to be strengthened by a three-dimensional network or 'scaffold' of another biodegradable polymer, poly(propylene fumarate) (PPF). PPF would be crosslinked with a biocompatible vinyl monomer, vinylpyrrolidone (VP). Three different approaches were tested to create dimensionally stable bone plates. First, via in situ crosslinking of PPF in the presence of PLGA. Secondly, by blending of precrosslinked PPF with PLGA. Finally, by simultaneous crosslinking and molding of the PLGA, PPF and VP. These were compared against extruded or compression molded PLGA controls. Results showed that compression molding at room temperature followed by crosslinking under pressure at elevated temperature and subsequently by gamma -irradiation appeared to yield the most favorable product as judged by swelling, hardness and flexural strength data. The composition of the implant material, PLGA(3):PPF(1):VP(0.7), appeared to be suitable and formed the compositional and procedural basis for in vivo biocompatibility studies. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:135 / 150
页数:16
相关论文
共 39 条
[1]   IN-VIVO DEGRADATION AND BIOCOMPATIBILITY STUDY OF IN-VITRO PRE-DEGRADED AS-POLYMERIZED POLYLACTIDE PARTICLES [J].
BERGSMA, JE ;
ROZEMA, FR ;
BOS, RRM ;
BOERING, G ;
DEBRUIJN, WC ;
PENNINGS, AJ .
BIOMATERIALS, 1995, 16 (04) :267-274
[2]   THE BIODEGRADABILITY OF POLYESTER BLENDS [J].
CHA, Y ;
PITT, CG .
BIOMATERIALS, 1990, 11 (02) :108-112
[3]  
Christel P, 1982, BIOMATERIALS 1980, P271
[4]   Finite element stress analysis of a hybrid fracture fixation plate [J].
Ferguson, SJ ;
Wyss, UP ;
Pichora, DR .
MEDICAL ENGINEERING & PHYSICS, 1996, 18 (03) :241-250
[5]   Resorbable device for fracture fixation: In vivo degradation and mechanical behaviour [J].
Fini, M ;
Giannini, S ;
Giardino, R ;
Giavaresi, G ;
Grimaldi, M ;
Aldini, NN ;
Orienti, L ;
Rocca, M .
INTERNATIONAL JOURNAL OF ARTIFICIAL ORGANS, 1995, 18 (12) :772-776
[6]   HISTOLOGICAL-EVALUATION OF BIODEGRADABLE AND NONDEGRADABLE MEMBRANES PLACED TRANSCUTANEOUSLY IN RATS [J].
GALGUT, P ;
PITROLA, R ;
WAITE, I ;
DOYLE, C ;
SMITH, R .
JOURNAL OF CLINICAL PERIODONTOLOGY, 1991, 18 (08) :581-586
[7]   INVIVO HISTOLOGIC AND BIOMECHANICAL CHARACTERIZATION OF A BIODEGRADABLE PARTICULATE COMPOSITE BONE-CEMENT [J].
GERHART, TN ;
RENSHAW, AA ;
MILLER, RL ;
NOECKER, RJ ;
HAYES, WC .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1989, 23 (01) :1-16
[8]   BIODEGRADABLE POLYMERS FOR USE IN SURGERY - POLYGLYCOLIC-POLY(ACTIC ACID) HOMOPOLYMERS AND COPOLYMERS .1. [J].
GILDING, DK ;
REED, AM .
POLYMER, 1979, 20 (12) :1459-1464
[9]   Mechanisms of polymer degradation and erosion [J].
Gopferich, A .
BIOMATERIALS, 1996, 17 (02) :103-114
[10]   IMMEDIATE IMPLANT PLACEMENT USING A BIODEGRADABLE BARRIER, POLYHYDROXYBUTYRATE-HYDROXYVALERATE REINFORCED WITH POLYGALACTIN-910 - AN EXPERIMENTAL-STUDY IN DOGS [J].
GOTFREDSEN, K ;
NIMB, L ;
HJORTINGHANSEN, E .
CLINICAL ORAL IMPLANTS RESEARCH, 1994, 5 (02) :83-91