Cooling rate influences in carbon fibre/PEEK composites. Part II: interlaminar fracture toughness

被引:117
作者
Gao, SL [1 ]
Kim, JK [1 ]
机构
[1] Hong Kong Univ Sci & Technol, Dept Mech Engn, Kowloon, Hong Kong, Peoples R China
关键词
adhesion; carbon fibre; fracture toughness; interface/interphase;
D O I
10.1016/S1359-835X(00)00188-3
中图分类号
T [工业技术];
学科分类号
08 [工学];
摘要
A study has been made of the effect of cooling rate on interlaminar fracture toughness of unidirectional carbon fibre-polyetheretherketone (PEEK) matrix composites. It is shown that the propagation values of both mode I and II propagation interlaminar fracture toughness increased with increasing cooling rate towards a saturation level for the range of cooling rate studied. The cooling rate dependency of the composite interlaminar fracture toughness is the result of complex interactions between two important properties, namely the matrix ductility and fibre-matrix interface bond strength. These two properties varied totally in an opposite manner against cooling rate through its effect on crystallinity: matrix ductility varied directly proportional to cooling rate while the converse is true for interface bond strength. The extent of plastic deformation of PEEK matrix contributed a predominant part to composite toughness, while an adequate interface bond is required to allow matrix deformation to take place to a full degree. A practical implication is that these two properties need to be optimised using an appropriate cooling rate to produce composites possessing high interlaminar fracture resistance. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:763 / 774
页数:12
相关论文
共 31 条
[1]
[2]
Bradley W. L., 1989, Key Engineering Materials, V37, P161
[3]
Carlsson L. A., 1986, Journal of Reinforced Plastics and Composites, V5, P170, DOI 10.1177/073168448600500302
[4]
INTERLAMINAR SHEAR FRACTURE OF LAMINATED COMPOSITES [J].
CHAI, H .
INTERNATIONAL JOURNAL OF FRACTURE, 1990, 43 (02) :117-131
[5]
INTERLAMINAR FRACTURE MORPHOLOGY OF CARBON-FIBER PEEK COMPOSITES [J].
CRICK, RA ;
LEACH, DC ;
MEAKIN, PJ ;
MOORE, DR .
JOURNAL OF MATERIALS SCIENCE, 1987, 22 (06) :2094-2104
[6]
CURTIS PT, 1987, P ICCM 6, V4, P401
[7]
A STUDY OF THE DELAMINATION RESISTANCE OF IM6/PEEK COMPOSITES [J].
DAVIES, P ;
CANTWELL, W ;
MOULIN, C ;
KAUSCH, HH .
COMPOSITES SCIENCE AND TECHNOLOGY, 1989, 36 (02) :153-166
[8]
Davies P, 1991, COMPOS MAT FATIGUE F, V3, P70
[9]
CRYSTALLIZATION AND FIBER MATRIX INTERACTION DURING THE MOLDING OF PEEK CARBON COMPOSITES [J].
DENAULT, J ;
VUKHANH, T .
POLYMER COMPOSITES, 1992, 13 (05) :361-371
[10]
Interphase research issues [J].
Fink, BK ;
McCullough, RL .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1999, 30 (01) :1-2