摘要
The AC impedance response of mixed ionic and electronic conductors (MIECs) is derived from first principles and quantitatively compared with experimental data. While the approach is not entirely new, the derivation is provided in a unified and comprehensive manner. Using Sm0.15Ce0.85O1.925-delta with Pt electrodes as a model system, a broad spectrum of electrical and thermodynamic properties is extracted solely from the measurement of impedance spectra over wide oxygen partial pressure and temperature ranges. Here, the oxygen partial pressure was varied from air [p(O2)=0.21 atm] to H-2 [p(O2)=10(-31) atm], and the temperature was varied from 500 degrees to 650 degrees C. It was essential for this analysis that the material under investigation exhibit, under some conditions, purely ionic behavior and, under others, mixed conducting behavior. The transition from ionic to mixed conducting behavior is recognizable not only from the oxygen partial pressure dependence of the total conductivity but also directly from the shape of the impedance spectra. Within the electrolytic regime, the impedance spectra (presented in Nyquist form) take the shape of simple, depressed arcs, whereas within the mixed conducting regime (under reducing conditions), the spectra exhibit the features associated with a half tear-drop-shaped element. Parameters derived from quantitative fitting of the impedance spectra include the concentration of free electron carriers, the mobilities and activation energies for both ion and electron transport, the electrolytic domain boundary, and the entropy and enthalpy of reduction. In addition, the electrochemical behavior of O-2 and H-2 at the Pt vertical bar ceria interface has been characterized from these measurements. Under oxidizing conditions, the data suggest an oxygen electrochemical reaction that is rate limited by the dissociated adsorption/diffusion of oxygen species on the Pt electrode, similar to Pt vertical bar YSZ (yttria-stabilized zirconia). Under reducing conditions, the inverse of the electrode resistivity obeys a p(O2)(-1/4) dependence, with an activation energy that is similar to that measured for the electronic conductivity. These results suggest that ceria is electrochemically active for hydrogen electro-oxidation and that the reaction is limited by the rate of removal of electrons from the ceria surface.
引用
收藏
页码:2979 / 2997
页数:19
相关论文
共 46 条
[21]  
Macdonald JR, 2005, IMPEDANCE SPECTROSCOPY: THEORY, EXPERIMENT, AND APPLICATIONS, 2ND EDITION, P1, DOI 10.1002/0471716243.ch1
[22]   THEORY OF SPACE-CHARGE POLARIZATION AND ELECTRODE-DISCHARGE EFFECTS [J].
MACDONALD, JR .
JOURNAL OF CHEMICAL PHYSICS, 1973, 58 (11) :4982-5001
[23]  
Minh NQ, 1995, SCI TECHNOLOGY CERAM, P41
[24]   ELECTRODE-REACTION AT PT,O-2(G)/STABILIZED ZIRCONIA INTERFACES .1. THEORETICAL CONSIDERATION OF REACTION MODEL [J].
MIZUSAKI, J ;
AMANO, K ;
YAMAUCHI, S ;
FUEKI, K .
SOLID STATE IONICS, 1987, 22 (04) :313-322
[25]   ELECTRODE-REACTION AT PT,O-2(G)/STABILIZED ZIRCONIA INTERFACES .2. ELECTROCHEMICAL MEASUREMENTS AND ANALYSIS [J].
MIZUSAKI, J ;
AMANO, K ;
YAMAUCHI, S ;
FUEKI, K .
SOLID STATE IONICS, 1987, 22 (04) :323-330
[26]   KINETICS OF THE ELECTRODE-REACTION AT THE H2-H2O POROUS PT STABILIZED ZIRCONIA INTERFACE [J].
MIZUSAKI, J ;
TAGAWA, H ;
ISOBE, K ;
TAJIKA, M ;
KOSHIRO, I ;
MARUYAMA, H ;
HIRANO, K .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1994, 141 (06) :1674-1683
[27]   Physical, chemical and electrochemical properties of pure and doped ceria [J].
Mogensen, M ;
Sammes, NM ;
Tompsett, GA .
SOLID STATE IONICS, 2000, 129 (1-4) :63-94
[28]   Steady-state, transient and small-amplitude AC responses of an electrochemical cell with immobile background charge: A network approach [J].
Moya, AA ;
Hayas, A ;
Horno, J .
SOLID STATE IONICS, 2000, 130 (1-2) :9-17
[30]  
RICHERT H, 1982, ELECTROCHEMISTRY SOL, P79