Low-temperature sintering and piezoelectric properties of ZnO-added 0.41Pb(Ni1/3 Nb2/3)O3-0.36PbTiO3-0.23PbZrO3 ceramics

被引:40
作者
Ahn, CW
Noh, SY
Nahm, S
Ryu, JH
Uchin, KJ
Yoon, SJ
Song, JS
机构
[1] Korea Univ, Dept Mat Sci & Engn, Seoul 136701, South Korea
[2] Penn State Univ, Mat Res Inst, Int Ctr Actuators & Transducers, University Pk, PA 16802 USA
[3] Korea Inst Sci & Technol, Thin Film Technol Res Ctr, Seoul 130650, South Korea
[4] Korea Electrotechnol Res Inst, Elect & Magnet Devices Grp, Chang Won 641120, South Korea
来源
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS | 2003年 / 42卷 / 9A期
关键词
0.41 Pb(Ni1/3Nb2/3)O-3-0.36PbTiO(3)-0.23PbZrO(3) ceramics; piezoelectric properties; low-temperature sintering;
D O I
10.1143/JJAP.42.5676
中图分类号
O59 [应用物理学];
学科分类号
摘要
The structure of 0.41(PbNi1/3Nb2/3)O-3-0.36PbTiO(3)-0.23PbZrO(3) (0.41PNN-0.36PT-0.23PZ) ceramics changed from pseudocubic to tetragonal when ZnO was added. For the specimens sintered above 1000degreesC, bulk density slightly decreased with the addition of ZnO but it significantly increased for the specimens sintered below 1000degreesC. Curie temperature (T,) and maximum dielectric constant increased when ZnO was added. Coercive electric field (E-c) and mechanical quality factor (Q) increased with the addition of ZnO but piezoelectric constant (d(33)), electromechanical coupling factor (k(p)) and dielectric constant (epsilon(3)(T)/epsilon(0)) decreased with the addition of ZnO for the specimens sintered above 1,000degreesC. However, for the specimens sintered below 1000degreesC, the addition of ZnO significantly improved the piezoelectric and dielectric constants, which could be due to the improvement of bulk density. The good dielectric and piezoelectric properties of d(33) = 525 (pC/N), k(p) = 0.53 and epsilon(3)(T)/epsilon(0) = 3400 were obtained for the specimen with 3 mol% ZnO sintered at 950degreesC for 1h.
引用
收藏
页码:5676 / 5680
页数:5
相关论文
共 9 条
[1]  
BANNO H, 1977, P 1 M FERR MAT THEIR, P339
[2]   The effects of Cd-substitution site on sintering behavior and electrical properties in Pb(Ni1/3Nb2/3)O-3-PbZrO3-PbTiO3 ceramics [J].
Cho, JH ;
Park, IE ;
Chung, HT ;
Kim, HG .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1997, 36 (1A) :181-187
[3]   Doping effects on the piezoelectric properties of low-temperature sintered PNN-PZT-based ceramics [J].
Chu, SY ;
Hsieh, CS .
JOURNAL OF MATERIALS SCIENCE LETTERS, 2000, 19 (07) :609-612
[4]   Piezoelectric properties of PbNi1/3Nb2/3O3-PbTiO3-PbZrO3 ceramics near the MPB [J].
Kondo, M ;
Hida, M ;
Tsukada, M ;
Kurihara, K ;
Kamehara, N .
JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1997, 105 (08) :719-721
[5]  
LUFF D, 1974, BRIT CERAM TRANS J, V73, P251
[6]   DENSIFICATION BEHAVIORS AND PIEZOELECTRIC PROPERTIES OF MNO2, SIO2-DOPED PB(NI1/3NB2/3)O3-PBTIO3-PBZRO3 CERAMICS [J].
MOON, JH ;
JANG, HM ;
YOU, BD .
JOURNAL OF MATERIALS RESEARCH, 1993, 8 (12) :3184-3191
[7]   FABRICATION OF PEROVSKITE LEAD MAGNESIUM NIOBATE [J].
SWARTZ, SL ;
SHROUT, TR .
MATERIALS RESEARCH BULLETIN, 1982, 17 (10) :1245-1250
[8]  
Uchino K., 1996, Piezoelectric Actuators and Ultrasonic Motors
[9]  
ZHILUN G, 1989, J AM CERAM SOC, V72, P486