3D fine scale ceramic components formed by ink-jet prototyping process

被引:136
作者
Noguera, R [1 ]
Lejeune, M [1 ]
Chartier, T [1 ]
机构
[1] ENSCI, SPCTS, UMR 6638, F-87065 Limoges, France
关键词
printing; suspensions; PZT;
D O I
10.1016/j.jeurceramsoc.2005.03.223
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Different investigations have been carried out to optimize an ink-jet printing technique, devoted to the fabrication of 3D fine scale ceramic parts, by adjustment of the fluid properties of the ceramic suspensions and by controlling the ejection and impact phenomena. A 10vol.% PZT loaded suspension characterized by a Newtonian behavior corresponding to a viscosity of 10 mPa s and to a ratio Re/We(1/2) of 5.98 has been selected. The ejection and impact phenomena strongly depend on the driving parameters of the printing head, in particular the formation of the droplet, with satellite or not, as well as its velocity and volume are function of the pulse amplitude. Moreover, the conditions of ejection (droplet velocity and volume) control the characteristics of the deposit (definition, spreading and thickness uniformity). Green PZT pillar array corresponding to the skeleton of 1-3 ceramic polyrner composite for imaging probes has been achieved by ink-jet printing with a definition equal to 90 mu m. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2055 / 2059
页数:5
相关论文
共 21 条
[1]   Freeform fabrication by controlled droplet deposition of powder filled melts [J].
Ainsley, C ;
Reis, N ;
Derby, B .
JOURNAL OF MATERIALS SCIENCE, 2002, 37 (15) :3155-3161
[2]  
BERTSCH A, 1998, J EUR CERAM SOC, V18, P583
[3]   PZT pillars for 1-3 composites prepared by ink-jet printing [J].
Bhatti, AR ;
Mott, M ;
Evans, JRG ;
Edirisinghe, MJ .
JOURNAL OF MATERIALS SCIENCE LETTERS, 2001, 20 (13) :1245-1248
[4]   THE COMPUTER-AIDED MANUFACTURE OF CERAMICS USING MULTILAYER JET PRINTING [J].
BLAZDELL, PF ;
EVANS, JRG ;
EDIRISINGHE, MJ ;
SHAW, P ;
BINSTEAD, MJ .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1995, 14 (22) :1562-1565
[5]   Stereolithography of structural complex ceramic parts [J].
Chartier, T ;
Chaput, C ;
Doreau, F ;
Loiseau, M .
JOURNAL OF MATERIALS SCIENCE, 2002, 37 (15) :3141-3147
[6]  
Doreau F, 2000, ADV ENG MATER, V2, P493, DOI 10.1002/1527-2648(200008)2:8<493::AID-ADEM493>3.0.CO
[7]  
2-C
[8]  
GUYOMAR D, 1994, P 2 JAP FRANC C MECH, P43
[9]   Stereolithography for the fabrication of ceramic three-dimensional parts [J].
Hinczewski, C. ;
Corbel, S. ;
Chartier, T. .
RAPID PROTOTYPING JOURNAL, 1998, 4 (03) :104-111
[10]   Fabrication of piezoelectric ceramic/polymer composite transducers using fused deposition of ceramics [J].
Lous, GM ;
Cornejo, IA ;
McNulty, TF ;
Safari, A ;
Danforth, SC .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2000, 83 (01) :124-128