摘要
The properties and performance of most bulk materials and coatings are controlled by interfaces. For bulk materials the surface is the most important interface, though grain and phase boundaries may also play a role in dictating performance. For coatings the coating-substrate interface is equally important and other internal interfaces may also contribute to behavior. This article reviews the effect of interfaces on the hardness of bulk materials, single and multilayer coatings highlighting the importance of engineering interfaces with high strength if coatings with optimum properties are to be achieved. A simple model is introduced which enables the effect of such interfaces to be more fully appreciated. The possibility of using graded compositions, such as ion implanted layers, to improve performance is also discussed in light of this model. (C) 2001 American Vacuum Society.
引用
收藏
页码:1404 / 1414
页数:11
相关论文
共 65 条
[1]   INFLUENCE OF POLYCRYSTAL GRAIN SIZE ON SEVERAL MECHANICAL PROPERTIES OF MATERIALS [J].
ARMSTRONG, RW .
METALLURGICAL TRANSACTIONS, 1970, 1 (05) :1169-+
[2]   Phenomenology of the size effect in hardness tests with a blunt pyramidal indenter [J].
Atkinson, M .
JOURNAL OF MATERIALS SCIENCE, 1998, 33 (11) :2937-2947
[3]   MECHANICAL-PROPERTIES OF COMPOSITIONALLY MODULATED AU-NI THIN-FILMS - NANOINDENTATION AND MICROCANTILEVER DEFLECTION EXPERIMENTS [J].
BAKER, SP ;
NIX, WD .
JOURNAL OF MATERIALS RESEARCH, 1994, 9 (12) :3131-3145
[4]   A COMPARISON OF 4 MICROINDENTATION HARDNESS TEST METHODS USING COPPER, 52100-STEEL, AND AN AMORPHOUS PD-CU-SI ALLOY [J].
BLAU, PJ .
METALLOGRAPHY, 1983, 16 (01) :1-18
[5]  
Bu''ckle H., 1959, Metall.Rev, V4, P49, DOI [10.1179/095066059790421746, DOI 10.1179/095066059790421746]
[6]  
Buckle H., 1973, The science of hardness testing and its research applications, P453
[7]   TECHNIQUES FOR IMPROVING THIN-FILM ADHESION [J].
BULL, SJ .
VACUUM, 1992, 43 (5-7) :517-520
[8]   AN EXPLANATION OF THE INDENTATION SIZE EFFECT IN CERAMICS [J].
BULL, SJ ;
PAGE, TF ;
YOFFE, EH .
PHILOSOPHICAL MAGAZINE LETTERS, 1989, 59 (06) :281-288
[9]   INDENTATION RESPONSE OF DIAMOND THIN-FILMS [J].
BULL, SJ ;
CHALKER, PR ;
JOHNSTON, C ;
COOPER, CV .
DIAMOND AND RELATED MATERIALS, 1994, 4 (01) :43-52
[10]   Multilayer coatings for improved performance [J].
Bull, SJ ;
Jones, AM .
SURFACE & COATINGS TECHNOLOGY, 1996, 78 (1-3) :173-184