Nano-scale study of the nucleation and growth of calcium phosphate coating on titanium implants

被引:138
作者
Barrere, F
Snel, MME
van Blitterswijk, CA
de Groot, K
Layrolle, P
机构
[1] IsoTis NV, NL-3720 AB Bilthoven, Netherlands
[2] Univ Twente, iBME, Enschede, Netherlands
[3] Univ Utrecht, NL-3508 TC Utrecht, Netherlands
[4] Leiden Univ, Biomat Res Grp, NL-2300 RA Leiden, Netherlands
[5] Fac Dent Surg, INSERM EM 9903, F-44042 Nantes, France
关键词
biomimetic coatings; amorphous calcium phosphate; Ti6A14V; atomic force microscopy (AFM); environmental scanning electronic microscopy (ESEM); nucleation; crystal growth; adhesion;
D O I
10.1016/j.biomaterials.2003.09.063
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The nucleation and growth of a calcium phosphate (Ca-P) coating deposited on titanium implants from simulated body fluid was investigated by using atomic force microscopy (AFM) and environmental scanning electron microscopy (ESEM). Forty titanium alloy plates were assigned into two groups. One group with a smooth surface having a maximum roughness R-max < 0.10 mum (s-Ti6Al4V) and a group with a rough surface with an R-max < 0.25 mum (r-Ti6Al4V) were used. Titanium samples were immersed in SBF concentrated by five (SBF x 5) from 10 min to 5 h and examined by AFM and ESEM. Scattered Ca-P deposits of approximately 15 nm in diameter appeared after only 10 min of immersion in SBF x 5. These Ca-P deposits grew up to 60-100 nm after 4 h on both s- and r-Ti6A14V substrates. With increasing immersion time, the packing of Ca-P deposits with size of tens of nanometers in diameter formed larger globules and then a continuous Ca-P film on titanium substrates. A direct contact between the Ca-P coating and the Ti6A14V surface was observed. The Ca-P coating was composed of nanosized deposits and of an interfacial glassy matrix. This interfacial glassy matrix might ensure the adhesion between the Ca-P coating and the Ti6A14V substrate. In the case of s-Ti6Al4V substrate. failures within this interfacial glassy matrix were observed overtime. Part of the glassy matrix remained on s-Ti6Al4V while part detached with the Ca-P film. The Ca-P coating detached from the smooth substrate, whereas the Ca-P film extended onto the whole rough titanium surface over time. In the case of r-Ti6A14V, the Ca-P coating covered evenly the substrate after immersion in SBF x 5 for 5 h. The present study suggested that the heterogeneous nucleation of Ca-P on titanium was immediate and did not depend on the Ti6A14V surface topography. The further growth and mechanical attachment of the final Ca-P coating strongly depended on the surface, for which a rough topography was beneficial. (C) 2003 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2901 / 2910
页数:10
相关论文
共 25 条
[21]  
Oyane A, 1999, BIOCERAMICS, V12, P157
[22]   SYNTHETIC AMORPHOUS CALCIUM-PHOSPHATE AND ITS RELATION TO BONE-MINERAL STRUCTURE [J].
POSNER, AS ;
BETTS, F .
ACCOUNTS OF CHEMICAL RESEARCH, 1975, 8 (08) :273-281
[23]  
TENGVALL P, 1992, Clinical Materials, V9, P115, DOI 10.1016/0267-6605(92)90056-Y
[24]   STUDY OF THE SURFACE CHARACTERISTICS OF MAGNETRON-SPUTTER CALCIUM-PHOSPHATE COATINGS [J].
WOLKE, JGC ;
VANDIJK, K ;
SCHAEKEN, HG ;
DEGROOT, K ;
JANSEN, JA .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1994, 28 (12) :1477-1484
[25]   Kinetics of nucleation and crystal growth of hydroxyapatite and fluorapatite on titanium oxide surfaces [J].
Wu, WJ ;
Nancollas, GH .
COLLOIDS AND SURFACES B-BIOINTERFACES, 1997, 10 (02) :87-94