摘要
Effects of cerium(III) ions are reported in this paper on the activity and hydrothermal stability of Cu-ZSM-5 catalysts for nitric oxide decomposition in water vapor-containing gas streams, Wet conditions drastically decrease the NO decomposition activity of unpromoted Cu-ZSM-5 catalysts at 500 degrees C. Activity is partially recovered upon removal of water vapor. Copper ion species migration leading to CuO formation inside the zeolite channels has been identified by STEM/EDX, XRD, and XPS as the major pathway to deactivation, The cerium modified Cu-ZSM-5 displays higher wet-gas activity for NO decomposition and recovers a higher fraction of its initial dry-gas activity than the Cu-ZSM-5 catalyst after removal of water vapor, The presence of cerium suppresses CuO particle formation and dealumination, providing higher hydrothermal stability for the zeolite structure and higher copper dispersion, all of which contribute to better catalytic performance of the Ce,Cu-ZSM-5 materials. (C) 1996 Academic Press, Inc.
引用
收藏
页码:131 / 145
页数:15
相关论文
共 37 条
[11]   IN-SITU ESR MONITORING OF CUH-ZSM-5 UP TO 500-DEGREES-C IN FLOWING DRY MIXTURES OF NO(NO2), C3H6(C2H5OH), AND EXCESS O-2 [J].
KUCHEROV, AV ;
GERLOCK, JL ;
JEN, HW ;
SHELEF, M .
JOURNAL OF CATALYSIS, 1995, 152 (01) :63-69
[12]   IN-SITU ESR MONITORING OF THE COORDINATION AND OXIDATION-STATES OF COPPER IN CU-ZSM-5 UP TO 500-DEGREES-C IN FLOWING GAS-MIXTURES .1. INTERACTION WITH HE, O-2, NO, NO2, AND H2O [J].
KUCHEROV, AV ;
GERLOCK, TL ;
JEN, HW ;
SHELEF, M .
ZEOLITES, 1995, 15 (01) :9-14
[13]  
LAGO RM, 1986, P 7 INT ZEOL C TOK, P667
[14]  
LEE CY, 1995, APPL CATAL B-ENVIRON, V5, P7
[15]   IDENTIFICATION OF COPPER(II) AND COPPER(I) AND THEIR INTERCONVERSION IN CU/ZSM-5 DE-NOX CATALYSTS [J].
LEI, GD ;
ADELMAN, BJ ;
SARKANY, J ;
SACHTLER, WMH .
APPLIED CATALYSIS B-ENVIRONMENTAL, 1995, 5 (03) :245-256
[16]  
LI Y, 1990, J PHYS CHEM-US, V94, P6148
[17]   TEMPERATURE-PROGRAMMED DESORPTION OF NITRIC-OXIDE OVER CU-ZSM-5 [J].
LI, YJ ;
ARMOR, JN .
APPLIED CATALYSIS, 1991, 76 (02) :L1-L8
[18]   CATALYTIC DECOMPOSITION OF NITRIC-OXIDE OVER CU-ZEOLITES [J].
LI, YJ ;
HALL, WK .
JOURNAL OF CATALYSIS, 1991, 129 (01) :202-215
[19]   TOTAL OXIDATION OF CARBON-MONOXIDE AND METHANE OVER TRANSITION METAL-FLUORITE OXIDE COMPOSITE CATALYSTS .2. CATALYST CHARACTERIZATION AND REACTION-KINETICS [J].
LIU, W ;
FLYTZANI-STEPHANOPOULOS, M .
JOURNAL OF CATALYSIS, 1995, 153 (02) :317-332
[20]   TOTAL OXIDATION OF CARBON-MONOXIDE AND METHANE OVER TRANSITION METAL-FLUORITE OXIDE COMPOSITE CATALYSTS .1. CATALYST COMPOSITION AND ACTIVITY [J].
LIU, W ;
FLYTZANI-STEPHANOPOULOS, M .
JOURNAL OF CATALYSIS, 1995, 153 (02) :304-316