Hydrogen and helium bubbles in silicon

被引:149
作者
Cerofolini, GF
Corni, F
Frabboni, S
Nobili, C
Ottaviani, G
Tonini, R
机构
[1] STMicroelect, I-95100 Catania, CT, Italy
[2] Ist Nazl Fis Mat, I-41100 Modena, MO, Italy
[3] Univ Modena, Dipartimento Fis, I-41100 Modena, MO, Italy
关键词
hydrogen; helium; silicon; defect-impurity interactions; precipitation; outdiffusion;
D O I
10.1016/S0927-796X(00)00007-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hydrogen is a quite common impurity in semiconductor-silicon technology: it is unintentionally but unavoidably added to the silicon after crystal growth during wafer processing, and continues to be present during wet oxidation, film depositions, etching and annealing steps. The effects of hydrogen in single crystal silicon at low concentration have been the subject of many papers, books and conference proceedings. Much less considered is the case of hydrogen at massive concentration. One Anal effect of heavy hydrogen loading is the formation of cavities and bubbles, with size up to 100 nm. Cavities and bubbles are also observed after helium loading by high-fluence ion implantation. This article reviews the basic mechanisms responsible for the formation and growth of such structures in single-crystalline silicon. In particular, starting from the loading (ion implantation) and having in mind the formation of the cavities, this paper will cover: the effects of substrate temperature, the interaction of vacancies and self-interstitials with the impurity, the mechanisms of gas segregation inside the cavities, the pressure which arises because of the segregation and the subsequent displacement field in the crystal, the stability against heat treatments of the gas in the cavities and of the cavities themselves. The understanding of the physical processes should lead to gain more insight in the processes of cleavage of the Si-Si bond and vacancy agglomeration which can induce not only the formation of cavities and bubbles, but also planar cutting or explosion. (C) 2000 Published by Elsevier Science S.A. All rights reserved.
引用
收藏
页码:1 / 52
页数:52
相关论文
共 100 条
  • [1] Blockage of the annealing-induced Si/SiO2 degradation by helium
    Afanas'ev, VV
    Stesmans, A
    [J]. APPLIED PHYSICS LETTERS, 1999, 74 (07) : 1009 - 1011
  • [2] Efficient production of silicon-on-insulator films by co-implantation of He+ with H+
    Agarwal, A
    Haynes, TE
    Venezia, VC
    Holland, OW
    Eaglesham, DJ
    [J]. APPLIED PHYSICS LETTERS, 1998, 72 (09) : 1086 - 1088
  • [3] 1ST-PRINCIPLES STUDY OF HE IN SI
    ALATALO, M
    PUSKA, MJ
    NIEMINEN, RM
    [J]. PHYSICAL REVIEW B, 1992, 46 (19): : 12806 - 12809
  • [4] BARTON TJ, 1990, ADV CHEM SER, P3
  • [5] Growth kinetics of a displacement field in hydrogen implanted single crystalline silicon
    Bisero, D
    Corni, F
    Frabboni, S
    Tonini, R
    Ottaviani, G
    Balboni, R
    [J]. JOURNAL OF APPLIED PHYSICS, 1998, 83 (08) : 4106 - 4110
  • [6] 1ST-PRINCIPLES CALCULATIONS OF DIFFUSION-COEFFICIENTS - HYDROGEN IN SILICON
    BLOCHL, PE
    VAN DE WALLE, CG
    PANTELIDES, ST
    [J]. PHYSICAL REVIEW LETTERS, 1990, 64 (12) : 1401 - 1404
  • [7] Structural and binding properties of vacancy clusters in silicon
    Bongiorno, A
    Colombo, L
    De la Rubia, TD
    [J]. EUROPHYSICS LETTERS, 1998, 43 (06): : 695 - 700
  • [8] ELECTRON-PARAMAGNETIC-RESONANCE OF MOLECULAR-HYDROGEN IN SILICON - COMMENT
    BROWER, KL
    MYERS, SM
    EDWARDS, AH
    JOHNSON, NM
    VAN DE WALLE, CG
    POINDEXTER, EH
    [J]. PHYSICAL REVIEW LETTERS, 1994, 73 (10) : 1456 - 1456
  • [9] CHEMICAL-KINETICS OF HYDROGEN AND (111) SI-SIO2 INTERFACE DEFECTS
    BROWER, KL
    MYERS, SM
    [J]. APPLIED PHYSICS LETTERS, 1990, 57 (02) : 162 - 164
  • [10] The history, physics, and applications of the Smart-Cut® process
    Bruel, M
    [J]. MRS BULLETIN, 1998, 23 (12) : 35 - 39