Corrosion of niobium in sulphuric and hydrochloric acid solutions at 75 and 95 °C

被引:75
作者
Asselin, Edouard [1 ]
Ahmed, Tawfik M. [1 ]
Alfantazi, Akram [1 ]
机构
[1] Univ British Columbia, Dept Mat Engn, Vancouver, BC V6T 1Z4, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
niobium; Pourbaix diagram; acid solution; polarization; gravimetric;
D O I
10.1016/j.corsci.2006.05.028
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
New Pourbaix diagrams were calculated at 25, 75 and 95 degrees C for the Nb-H2O system. The species Nb(OH)(4)(+) and NbO3- were considered. Potentiodynamic polarization and mass loss experiments (14 days) were conducted in concentrated H2SO4 (20, 40 and 80 wt%) and HCl (20 and 38 wt%) solutions at 75 and 95 degrees C. Nb forms a metastable pentoxide (Nb2O5) in H2SO4 and HCl solutions which dissolves as Nb(OH)(4)(+). Corrosion rates decrease between the 40% and the 80% H2SO4 solutions. SEM micrographs show generalized pitting in the 20% and 40% H2SO4 solutions. Mass loss corrosion rates did not exceed 306 mu m/yr. Corrosion rates estimated by Tafel extrapolation were within two orders of magnitude of those measured by mass loss and it is shown that this finding is consistent with the thickening of the oxide. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:694 / 710
页数:17
相关论文
共 34 条
[1]  
*ASTM, G311990 ASTM, V3
[2]  
BARD AJ, 1985, STANDARD CHEM POTENT, P527
[3]   IONIC HYDRATION AND SINGLE ION ACTIVITIES IN UNASSOCIATED CHLORIDES AT HIGH IONIC STRENGTHS [J].
BATES, RG ;
STAPLES, BR ;
ROBINSON, RA .
ANALYTICAL CHEMISTRY, 1970, 42 (08) :867-&
[4]  
Bishop C R, 1963, CORROSION ENG, V19, P308
[5]  
BOCKRIS JO, 1970, MODERN ELECTROCHEMIS, V2, pCH9
[6]  
Brubaker S. K., 1987, ASM HDB CORROSION, V13, P1148
[7]  
Bulhoes LOS, 1984, P 11 INT C MET CORR, V3, P437
[8]  
BURNS RH, 1984, ASTM STP, V849, P50
[9]   THE CORROSION BEHAVIOR OF NIOBIUM IN HYDROCHLORIC-ACID SOLUTIONS [J].
COVINO, BS ;
CARTER, JP ;
CRAMER, SD .
CORROSION, 1980, 36 (10) :554-558